| Density | 8.14 g/cm³ |
| Melting Range | 1280-1345°C |
| Name | Incoloy 901 |
| Tensile Strength | Up to 1380 MPa (200 ksi) at room temperature |
| Yield Strength | 1000 MPa (145 ksi) at room temperature |
| Elongation | 20-30% |
| Hardness (HB) | 277-302 HB |
| Thermal Conductivity | 10.3 W/m·K at 100°C |
| Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.12 µΩ·m at 20°C |
| Modulus of Elasticity | 196 GPa (28.4 x 10^6 psi) |
| Magnetic Properties | Non-magnetic |
| Packaging Details | Standard export packaging, or packaging as required |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Ability | 5000 tons per month |
| Model Number | Incoloy 901 alloy |
| Place of Origin | China |
| Brand Name | Zhonggong Special Metallurgy |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
Incoloy 926 Corrosion Resistant Alloy High Strength UNS N08926 Light Rod And
926 Nickel Based Alloy Steel Rods Excellent Processing Alloy 1.4529 Tubes
Oxidation Resistant Incoloy 800HT Alloy Bar With Enhanced Thermal Stability
8.14g/cm3 Nickel Based Alloy 925 Round Bar Incoloy 925 Alloy
Product Specification
| Density | 8.14 g/cm³ | Melting Range | 1280-1345°C |
| Name | Incoloy 901 | Tensile Strength | Up to 1380 MPa (200 ksi) at room temperature |
| Yield Strength | 1000 MPa (145 ksi) at room temperature | Elongation | 20-30% |
| Hardness (HB) | 277-302 HB | Thermal Conductivity | 10.3 W/m·K at 100°C |
| Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) | Electrical Resistivity | 1.12 µΩ·m at 20°C |
| Modulus of Elasticity | 196 GPa (28.4 x 10^6 psi) | Magnetic Properties | Non-magnetic |
| Packaging Details | Standard export packaging, or packaging as required | Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Model Number | Incoloy 901 alloy | Place of Origin | China |
| Brand Name | Zhonggong Special Metallurgy | Certification | ISO Certificate |
| High Light | Incoloy 901 Alloy ,Incoloy Alloy 901 | ||
Incoloy 901 Alloy: High-Strength Nickel-Iron-Chromium Superalloy For Demanding Applications
Product Description of Incoloy 901 Alloy:
Incoloy 901 alloy is a precipitation-hardening nickel-iron-chromium superalloy known for its exceptional strength and high resistance to corrosion and oxidation at elevated temperatures. It derives its strength primarily from additions of aluminum and titanium, which precipitate upon aging. This alloy exhibits excellent mechanical properties, including high tensile and yield strength, coupled with good ductility and toughness.
Incoloy 901 finds extensive use in aerospace applications, particularly in gas turbine engines and components subjected to high temperatures and mechanical stress. Its superior resistance to stress-corrosion cracking and oxidation makes it ideal for critical parts such as turbine discs, shafts, and fasteners.
The alloy's ability to maintain strength and integrity at temperatures up to approximately 650°C (1200°F) makes it suitable for both static and rotating components in jet engines and industrial gas turbines. Additionally, its non-magnetic properties and reliable performance in harsh environments contribute to its widespread adoption in demanding engineering applications.
In summary, Incoloy 901 alloy is prized for its combination of high strength, excellent corrosion resistance, and thermal stability, making it a preferred material where reliability and performance under extreme conditions are paramount.
Here's a table detailing the chemical composition of Incoloy 901 alloy:
| Element | Percentage Range |
|---|---|
| Nickel (Ni) | 42-46% |
| Iron (Fe) | 33-38% |
| Chromium (Cr) | 11-14% |
| Titanium (Ti) | 2.6-3.4% |
| Aluminum (Al) | 0.35-0.75% |
| Manganese (Mn) | 0.0-0.35% |
| Silicon (Si) | 0.0-0.4% |
| Sulfur (S) | 0.0-0.02% |
| Copper (Cu) | 0.0-0.2% |
| Carbon (C) | 0.0-0.1% |
| Cobalt (Co) | 0.0-0.1% |
| Phosphorus (P) | 0.0-0.015% |
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company
Year Established:
2010
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Active Member
Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...
Get in touch with us
Leave a Message, we will call you back quickly!