| Density | ~8.3 g/cm³ |
| Melting Point | ~1400°C (2550°F) |
| Thermal Conductivity | ~11-13 W/m·K |
| Yield Strength | ~850 MPa (123 ksi) |
| Ultimate Tensile Strength | ~1000 MPa (145 ksi) |
| Elongation | ~12% |
| Hardness (Rockwell) | ~HRB 95-100 |
| Applications | Aerospace components, gas turbines, and high-temperature engines |
| Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH4169 alloy |
| Place of Origin | China |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
Incoloy 926 Corrosion Resistant Alloy High Strength UNS N08926 Light Rod And
926 Nickel Based Alloy Steel Rods Excellent Processing Alloy 1.4529 Tubes
Oxidation Resistant Incoloy 800HT Alloy Bar With Enhanced Thermal Stability
8.14g/cm3 Nickel Based Alloy 925 Round Bar Incoloy 925 Alloy
Product Specification
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
| Density | ~8.3 g/cm³ | Melting Point | ~1400°C (2550°F) |
| Thermal Conductivity | ~11-13 W/m·K | Yield Strength | ~850 MPa (123 ksi) |
| Ultimate Tensile Strength | ~1000 MPa (145 ksi) | Elongation | ~12% |
| Hardness (Rockwell) | ~HRB 95-100 | Applications | Aerospace components, gas turbines, and high-temperature engines |
| Brand Name | Zhonggong Special Metallurgy | Model Number | GH4169 alloy |
| Place of Origin | China | Certification | ISO Certificate |
| High Light | High Strength Ni Based Superalloy ,GH4169 Ni Based Superalloy | ||
GH4169 Alloy
GH4169 is a high-performance nickel-based superalloy specifically designed for excellent strength and stability at elevated temperatures. It is widely used in demanding applications requiring exceptional thermal and oxidative resistance.
Key Features:
GH4169’s combination of high strength, thermal stability, and corrosion resistance makes it an ideal choice for applications requiring reliable performance under severe conditions.
This description emphasizes the key properties and typical uses of GH4169 alloy, highlighting its suitability for high-performance applications.
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company
Year Established:
2010
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Active Member
Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...
Get in touch with us
Leave a Message, we will call you back quickly!