Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Ability | 5000 tons per month |
Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
Packaging Details | Standard export packaging, or packaging as required |
Density | ~8.3 g/cm³ |
Melting Point | ~1390°C (2530°F) |
Thermal Conductivity | ~11-12 W/m·K |
Yield Strength | ~700 MPa (102 ksi) |
~700 MPa (102 ksi) | 900 MPa (130 ksi) |
Elongation | ~10% |
Hardness (Rockwell) | ~HRB 90-95 |
Applications | Aerospace components, gas turbines, and high-temperature industrial parts |
Brand Name | Zhonggong Special Metallurgy |
Model Number | GH4145 alloy |
Place of Origin | China |
Certification | ISO Certificate |
View Detail Information
Explore similar products
Incoloy 926 Corrosion Resistant Alloy High Strength UNS N08926 Light Rod And
926 Nickel Based Alloy Steel Rods Excellent Processing Alloy 1.4529 Tubes
Oxidation Resistant Incoloy 800HT Alloy Bar With Enhanced Thermal Stability
8.14g/cm3 Nickel Based Alloy 925 Round Bar Incoloy 925 Alloy
Product Specification
Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
Density | ~8.3 g/cm³ | Melting Point | ~1390°C (2530°F) |
Thermal Conductivity | ~11-12 W/m·K | Yield Strength | ~700 MPa (102 ksi) |
~700 MPa (102 ksi) | 900 MPa (130 ksi) | Elongation | ~10% |
Hardness (Rockwell) | ~HRB 90-95 | Applications | Aerospace components, gas turbines, and high-temperature industrial parts |
Brand Name | Zhonggong Special Metallurgy | Model Number | GH4145 alloy |
Place of Origin | China | Certification | ISO Certificate |
High Light | Nickel Based Superalloy GH4145 ,Ni Based Superalloy GH4145 |
GH4145 Alloy
GH4145 is a high-performance nickel-based superalloy renowned for its exceptional strength, thermal stability, and resistance to oxidation and corrosion. It is designed for use in demanding high-temperature environments where reliability and durability are critical.
Key Features:
GH4145 alloy’s superior combination of strength, thermal resistance, and corrosion protection makes it an ideal material for critical applications that require reliable performance in challenging conditions.
Here’s a detailed composition table for GH4145 alloy:
Element | Content Range |
---|---|
Nickel (Ni) | Balance |
Chromium (Cr) | 18.0-21.0% |
Iron (Fe) | 14.0-17.0% |
Cobalt (Co) | 8.0-10.0% |
Molybdenum (Mo) | 2.0-3.0% |
Titanium (Ti) | 1.5-2.5% |
Aluminum (Al) | 1.0-1.5% |
Boron (B) | 0.005-0.015% |
This table provides a clear overview of the chemical composition of GH4145 alloy, detailing the content ranges of its key elements.
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company
Year Established:
2010
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...
Get in touch with us
Leave a Message, we will call you back quickly!