| Payment Terms | T/T, L/C |
| Supply Ability | 1000TONS/MONTH |
| Delivery Time | 5-8 Work Days |
| Packaging Details | Plywood Boxes |
| Alloys | TP316L |
| Certificate | ASME BPE |
| O.D. Range | 1/4'' (6.35MM) - 6'' (152.4MM) |
| W.T. Range | 0.065''(1.65MM) - 0.109''(2.77MM) |
| Finish | BA, MP,EP |
| Mill Test Certificate | EN10204 3.1 |
| Brand Name | SPEZILLA |
| Model Number | 1/4'' - 6'' |
| Certification | ASME BPE |
| Place of Origin | CHINA |
View Detail Information
Explore similar products
Seamless High Purity Stainless Steel Tubing Custom Lengths / Sizes 0.4um Surface
Seamless 316 Stainless Steel Tubing , Electropolished Stainless Steel Tubing
ASTM A270 Welded High Purity Stainless Steel Tubing TP316L Smooth Surface
Polished Stainless Tube , 2 Inch Stainless Steel Tubing For Pharmatheutical
Product Specification
| Payment Terms | T/T, L/C | Supply Ability | 1000TONS/MONTH |
| Delivery Time | 5-8 Work Days | Packaging Details | Plywood Boxes |
| Alloys | TP316L | Certificate | ASME BPE |
| O.D. Range | 1/4'' (6.35MM) - 6'' (152.4MM) | W.T. Range | 0.065''(1.65MM) - 0.109''(2.77MM) |
| Finish | BA, MP,EP | Mill Test Certificate | EN10204 3.1 |
| Brand Name | SPEZILLA | Model Number | 1/4'' - 6'' |
| Certification | ASME BPE | Place of Origin | CHINA |
| High Light | electropolished stainless steel pipe ,316 ss tubing | ||
High Purity Stainless Sanitary Tubing ASME BPE Industrial Stainless Steel Pipe
Description:
Mechanically Polished or Electropolished high purity stainless steel sanitary tubing for use in pharmaceutical, semi conductor, biotechnology and other high purity processes.
Our high purity stainless steel sanitary tubing is manufactured to the stringent ASME BPE and ASTM A270 S2 standards making it ideal for most high purity applications.
1. Mechanically Polished SF1 Finish
Guaranteed 0.8um max OD, 0.51um max ID
Our SF1 high purity stainless steel sanitary tubing is fully boroscoped and mechanically polished on both the ID and OD surfaces thus minimizing surface finish anomalies and reducing customer inspection requirements.
2. Electropolished SF4 Finish
Guaranteed 0.8um Max OD, 0.38um max ID after EP
Our SF4 high purity stainless steel sanitary tubing gives and ultra-smooth, corrosion resistant, chromium, enriched surface where contaminants cannot hide. This EP tube is processed ad packaged in a certified ISO Class 5 clean room - a must for tubing used in high purity environments.
1. AISI 316L TIG welded, grounded and extruded, according to ASTM A270 specifications.
2. Tubing are manufactured and tested according to ASTM A270 tolerances A269.
3. Outside permanently marked with heat number for identification.
4. Inside finishing Ra <0,5 µm, outside finishing Ra <0,8 µm (electropolished on request).
5. Tubing to be passivated and rinsed with deionized water after polishing.
6. Tubing to be end capped, paper or plastic sleeved and placed in nylon sheet.
7. Available in 6 meters nominal length.
8. Test report (MTR) like chemical analysis certificates with heat number and roughness test are supplied on request and have to be requested at order issue with the tubing.
Specifications:
| ASME BPE High Purity Stainless Steel Sanitary Tubing | |||||||||||||
| OD(INCH) | 0.236'' | 0.315'' | 0.25'' | 0.38'' | 0.50'' | 0.75'' | 1.00'' | 1.50'' | 2.00'' | 2.50'' | 3.00'' | 4.00'' | 6.00'' |
| OD(MM) | 6.0 | 8.0 | 6.35 | 9.53 | 12.7 | 19.05 | 25.4 | 38.1 | 50.8 | 63.5 | 76.2 | 101.6 | 152.4 |
| ID(MM) | 4.0 | 6.0 | 4.57 | 7.75 | 9.5 | 15.85 | 22.2 | 34.9 | 47.6 | 60.3 | 73.0 | 97.6 | 147.1 |
| WT(MM) | 1.0 | 1.0 | 0.9 | 0.9 | 1.6 | 1.6 | 1.6 | 1.6 | 1.6 | 1.6 | 1.6 | 2.0 | 2.7 |
| SWG | N/A | N/A | 20 | 20 | 16 | 16 | 16 | 16 | 16 | 16 | 16 | 14 | 12 |
Applications:
For the dairy, food, beverage, pharmacutical, BPE and other markets.
Spezilla's high purity stainless steel sanitary tubing exceeds the high standards in the industry, The ID is mechanically polished(M.P.) to 20Ra(0.5µm) finished or special cold drawing plus cold pilger and bright anealed special processed to 15Ra(0.4µm) finished to meet ASTM A270, and BPE standards.
Each tube is eddy current tested to conform to ASTM A249 follow by specialized cleaning and packaging to maintain contaminant-free tubing.
![]()
Company Details
Business Type:
Manufacturer,Exporter
Year Established:
2011
Total Annual:
>3000000.00
Ecer Certification:
Verified Supplier
Spezilla specialise in manufacturing high quality precision stainless steel tube and other corrosion resistant alloy tubes that are designed to industry and customer specifications. Our products are manufactured to the highest quality standards and are very competitively priced. Our mission is to pr... Spezilla specialise in manufacturing high quality precision stainless steel tube and other corrosion resistant alloy tubes that are designed to industry and customer specifications. Our products are manufactured to the highest quality standards and are very competitively priced. Our mission is to pr...
Get in touch with us
Leave a Message, we will call you back quickly!