China Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for
China Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for

  1. China Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for
  2. China Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for
  3. China Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for
  4. China Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for

Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for

  1. MOQ: 500 kgs
  2. Price: 22 - 30 USD/Kg
  3. Get Latest Price
Payment Terms L/C, T/T, Western Union
Supply Ability 3 Ton per week
Delivery Time 5 - 12 days based on the quantity
Packaging Details standard packing for export
Products Nickel Alloy Sheet & Plate
Grade Inconel 718
Thickness 0.5 - 30.0mm
Standard size 1000*2000mm 1219*2438mm
Standard ASTM EN
Service Cutting
Loading Port Shanghai Port
Surface 2B NO.1
Brand Name DELTA
Model Number Inconel 718
Certification ISO
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C, T/T, Western Union Supply Ability 3 Ton per week
Delivery Time 5 - 12 days based on the quantity Packaging Details standard packing for export
Products Nickel Alloy Sheet & Plate Grade Inconel 718
Thickness 0.5 - 30.0mm Standard size 1000*2000mm 1219*2438mm
Standard ASTM EN Service Cutting
Loading Port Shanghai Port Surface 2B NO.1
Brand Name DELTA Model Number Inconel 718
Certification ISO Place of Origin China
High Light Inconel 718 nickel alloy plate ,solution annealed nickel chromium plate ,machinable Inconel 718 superalloy

Inconel 718 Nickel-Chromium Superalloy Plate Solution Annealed & Ready for Machining

 

Products Specification

 

Products Name Inconel 718  Nickel Alloy Sheet Plate
Thickness Cold rolled: 0.5 - 3.0mm   Hot rolled 4.0 - 30.0mm
Standard Size 1000*2000mm 1219*2438mm 1219*3048mm 1500*6000mm
Surface 2B NO.1
MOQ 50 kgs
Service Cutting, Surface Finishing
Packing  Waterproof paper and wooden pallets
Loading Port Shanghai Port
Price term FOB  CFR CIF EXW
Payment term 30% TT in advance , 70% TT balance against copy of B/L
Main Grade Hastelloy C22 C4 X  C276 G35
Monel 400 K500
Incoloy 800 800H 800HT 825  925
Inconel 600 601 617 625 716 718
Stainless  Steel Grade 201 202 301 304L 309S 310S 316L 316Ti 317L 321 347 409L 410 410S 420J1 420J2 430 431 436L 439 440A/B/C 441 443 444 2205 2507 904L 254SMO 253MA

 

Inconel 718 Nickel-Chromium Superalloy Plate – Solution Annealed & Ready for Machining

Engineered for demanding aerospace, oil & gas, and power generation applications, solution-annealed Inconel 718 nickel-chromium superalloy plate offers the ideal balance of ductility, corrosion resistance, and machinability—serving as the preferred starting condition for complex, high-precision components. Unlike precipitation-hardened (aged) material, the solution-annealed condition maximizes formability and reduces tool wear during machining, while retaining the alloy’s inherent resistance to oxidation, sulfidation, and stress corrosion cracking.

This product guide provides detailed technical data, processing advantages, industry standards, and application insights for Inconel 718 plate supplied in the solution-annealed (UNS N07718, AMS 5662/5596 compliant) condition, optimized for secondary fabrication and final heat treatment.


Why Choose Solution-Annealed Inconel 718 Plate?

Inconel 718 derives its legendary strength from gamma-double-prime (γ″) and gamma-prime (γ′) precipitates formed during aging. However, these hard phases also increase hardness and reduce machinability. By supplying the material in the solution-annealed condition, manufacturers benefit from:

  • Enhanced ductility and reduced hardness (typically 25–35 HRC vs. 40+ HRC in aged condition)
  • Lower cutting forces and extended tool life during milling, turning, and drilling
  • Improved cold-forming capability for bending, stamping, or deep drawing
  • Uniform microstructure free of residual stresses from prior processing
  • Flexibility to perform final aging after machining, minimizing distortion

This makes solution-annealed plate the standard choice for shops producing turbine blades, downhole tools, fasteners, and custom aerospace fittings.


Material Standards & Designations

Parameter Specification
UNS Number N07718
Werkstoff Number 2.4668
Common Names Alloy 718, GH4169, Nickel 718
ASTM B670 (plate/sheet)
AMS (Aerospace) AMS 5662 (bar/plate), AMS 5596 (sheet) – solution-annealed variant
ASME Section II, Part D; BPVC Code Case 2222-1
NACE MR0175 / ISO 15156 Qualified for sour service environments

All plates are fully traceable with Mill Test Reports (MTRs) including chemistry, mechanical properties, and heat treatment certification.


Chemical Composition (Weight %)

Element Typical Range
Nickel (Ni) 50.0 – 55.0
Chromium (Cr) 17.0 – 21.0
Iron (Fe) Balance
Niobium (Nb) + Tantalum (Ta) 4.75 – 5.50
Molybdenum (Mo) 2.80 – 3.30
Titanium (Ti) 0.65 – 1.15
Aluminum (Al) 0.20 – 0.80
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 0.35
Silicon (Si) ≤ 0.35
Sulfur (S) ≤ 0.015
Phosphorus (P) ≤ 0.015
Copper (Cu) ≤ 0.30
Cobalt (Co) ≤ 1.00

Note: Nb and Ti remain in solid solution after annealing—precipitation occurs only during subsequent aging.


Solution Annealing Process (Per ASTM B670 / AMS Guidelines)

The plate is heated to 954–982°C (1750–1800°F), held for sufficient time (typically 1 hour per inch of thickness), then rapidly cooled (air or water quench) to:

  • Dissolve γ″ and γ′ strengthening phases
  • Homogenize the microstructure
  • Maximize ductility and corrosion resistance
  • Prepare the material for optimal response to final aging

This condition is often designated as “Condition A” in procurement specifications.


Mechanical Properties – Solution Annealed Condition

Property Metric Imperial
Tensile Strength 965–1100 MPa 140–160 ksi
Yield Strength (0.2% offset) 550–760 MPa 80–110 ksi
Elongation ≥ 30% ≥ 30%
Hardness 25–35 HRC —
Reduction of Area ≥ 35% —

Compared to aged material, yield strength is ~30% lower—but machinability improves by 40–60%.


Physical Properties

Property Value
Density 8.19 g/cm³ (0.296 lb/in³)
Melting Range 1260–1336°C (2300–2437°F)
Thermal Conductivity (100°C) 11.4 W/m·K
Specific Heat 435 J/kg·K
Electrical Resistivity 1.25 µΩ·m
Coefficient of Thermal Expansion (20–100°C) 12.7 × 10⁻⁶ /°C

Excellent thermal stability supports consistent performance during machining and subsequent heat treatment.


Available Dimensions & Tolerances

Form Thickness Range Width Length Tolerance (Typical)
Plate 6.0 mm – 100+ mm 1000–2000 mm 2000–6000 mm ±0.15 mm (per ASTM B670)
Sheet 0.5 – 6.0 mm 600–1500 mm 1000–3000 mm ±0.05 mm
  • Surface Finish: Hot-rolled descaled, pickled, or cold-rolled bright annealed
  • Edge Condition: Mill edge or slit edge (deburred available)
  • Custom Cutting: Waterjet, laser, or saw-cut to print

Key Advantages for Machining Operations

  1. Reduced Work Hardening Rate: Softer matrix minimizes rapid tool dulling.
  2. Better Chip Control: Improved ductility allows for continuous chip formation.
  3. Lower Power Consumption: Reduced cutting forces extend spindle life.
  4. Complex Geometry Feasibility: Ideal for 5-axis milling of turbine airfoils or impellers.
  5. Post-Machining Aging: Final heat treatment achieves full strength with minimal distortion.

Recommended Machining Practices:

  • Tooling: Carbide inserts (ISO K or S class), sharp edges, positive rake angles
  • Coolant: High-pressure soluble oil or synthetic coolant
  • Speeds: 15–30 m/min (50–100 SFM) for turning/milling
  • Feeds: 0.1–0.3 mm/rev (0.004–0.012 in/rev)
  • Avoid: Interrupted cuts without proper tool support

Common Applications (Machined from Solution-Annealed Plate)

Industry Components
Aerospace Turbine blades, compressor hubs, fuel system manifolds, landing gear bushings
Oil & Gas Downhole safety valves, choke stems, subsea connector bodies
Power Generation Gas turbine nozzles, combustor liners, steam valve stems
Defense Rocket motor casings, missile guidance housings
Industrial High-pressure reactor internals, cryogenic flanges, precision springs

After machining, parts are typically aged per AMS 5662 (718°C/8h + 621°C/8h) to achieve final mechanical properties.


Quality Assurance & Certification

Every batch includes:

  • Full chemical analysis (OES or ICP)
  • Tensile test report (room temperature)
  • Hardness verification (Rockwell C)
  • Ultrasonic inspection (optional per AMS 2631)
  • EN 10204 3.1 or 3.2 compliance documentation
  • AS9100/ISO 9001 quality system certification

Storage & Handling Recommendations

  • Store in dry, climate-controlled environment to prevent surface oxidation
  • Use non-metallic slings or padded lifters to avoid surface damage
  • Keep separate from carbon steel to prevent iron contamination (which can initiate pitting)
  • Clean with alkaline cleaners before welding or heat treatment

Conclusion

Solution-annealed Inconel 718 plate is not just a raw material—it’s a strategic enabler of manufacturing efficiency and part integrity. By beginning fabrication in this soft, ductile condition, engineers reduce scrap rates, improve throughput, and ensure that final-aged components meet stringent aerospace and industrial performance criteria.

Whether you’re machining a single prototype or launching high-volume production, solution-annealed Inconel 718 delivers the optimal blend of workability and ultimate performance.


Contact us today for certified, ready-to-machine Inconel 718 plate in standard or custom sizes—with full documentation, global shipping, and technical support from metallurgy experts.

solution annealed Inconel 718 plate, machinable Inconel 718 sheet, UNS N07718 soft condition, Inconel 718 for CNC machining, AMS 5662 solution treated plate, ductile nickel superalloy plate, Inconel 718 pre-machining condition, high-strength alloy ready for aging, aerospace Inconel plate supplier, corrosion resistant nickel plate for fabrication

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Exporter

  • Total Annual:

    >1000000

  • Employee Number:

    >100

  • Ecer Certification:

    Verified Supplier

Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative... Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative...

+ Read More

Get in touch with us

  • Reach Us
  • JIANGSU MITTEL STEEL INDUSTRIAL LIMITED
  • No.283-1, Youyi Middle Road, Xishan District, Wuxi City, Jiangsu Province
  • https://www.stainless-strips.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement