China Hot Rolled Incoloy 800 HT Plate 6mm Thick X 1500mm Width Nickel-Iron-Chromium
China Hot Rolled Incoloy 800 HT Plate 6mm Thick X 1500mm Width Nickel-Iron-Chromium

  1. China Hot Rolled Incoloy 800 HT Plate 6mm Thick X 1500mm Width Nickel-Iron-Chromium

Hot Rolled Incoloy 800 HT Plate 6mm Thick X 1500mm Width Nickel-Iron-Chromium

  1. MOQ: 100 kg
  2. Price: US $3.65-12.85 / kg
  3. Get Latest Price
Material Grade Incoloy 800 HT
Shape Flat
Technique Hot Rolled
Surface Treatment Polished
Thickness Range 0.3mm to 120mm
Width Range 1000mm to 2000mm
Length Range 1000mm to 6000mm
Iron Content 39.5% min
Nickel Content 30-35%
Chromium Content 19-23%
Aluminum + Titanium 0.85-1.20%
Carbon Content 0.06-0.10%
Max Temperature 1100°F (600°C)
Production Capacity 500000kgs
Edge Type Mill edge and slit edge
Certification AISI, ASTM

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Material Grade Incoloy 800 HT Shape Flat
Technique Hot Rolled Surface Treatment Polished
Thickness Range 0.3mm to 120mm Width Range 1000mm to 2000mm
Length Range 1000mm to 6000mm Iron Content 39.5% min
Nickel Content 30-35% Chromium Content 19-23%
Aluminum + Titanium 0.85-1.20% Carbon Content 0.06-0.10%
Max Temperature 1100°F (600°C) Production Capacity 500000kgs
Edge Type Mill edge and slit edge Certification AISI, ASTM
High Light Hot Rolled Incoloy 800 HT Plate6mm Thick Nickel-Iron-Chromium Alloy Plate1500mm Width Superalloy Plate
Incoloy 800HT Plate - 6mm Thick x 1500mm x 6000mm Hot Rolled
Incoloy 800/800H/HT is an austenitic superalloy widely used in high-temperature pressure-bearing structural components. This nickel-iron-chromium alloy offers excellent corrosion resistance to nitric acid, organic acids, and various corrosive environments including water, vapor, steam, air, and carbon dioxide mixtures.
Product Specifications
TechniqueHot Rolled and Cold Rolled
TypePlate, Coil, Strip
ThicknessHot rolled: 0.3mm to 3mm
Cold rolled: 3mm to 120mm
Width1000mm, 1500mm, 2000mm or customized
Length1000mm to 6000mm or customized
StandardASTM A240, ASTM A167, JIS, SUS, EN, DIN, GB, etc
EdgeMill edge and slit edge
Material GradeMonel 400, Monel K-500, Monel R405
Applications
Aerospace, shipbuilding, petroleum, chemical industry, nuclear power, electronics, steam turbine, high-speed rail, marine engineering, pressure vessels
Certification & Quality
ISO9001 certified with Material Test Certificates (MTC) available. All products come with material test reports meeting normal industry standards.
Ordering Information
MOQ1 Ton per specification
IncotermEXW, FOB, CIF, CFR
Loading PortShanghai Port
ShippingFCL, LCL, Bulk Ship, Express
Delivery7-10 days for stock, 15-20 days for production
Capacity500 tons per year
Available Product Forms
Alloy Bar, Alloy Plate, Alloy Sheet, Alloy Pipe, Alloy Pipe Fittings, Alloy Flanges, Alloy Tube, Alloy Weld Wire
Incoloy 800HT Chemical Composition
ElementComposition
Fe39.5% min
Ni30-35%
Cr19-23%
Al+Ti0.85-1.20%
C0.06-0.10%
Key Characteristics
  • Excellent resistance to oxidation, sulfidation, and carburization
  • Higher creep and rupture properties for high temperature situations above 1100°F (600°C)
  • Resistant to high temperature corrosion and prolonged exposure
  • Readily machined by standard methods
  • Resistance to aqueous corrosion at moderate temperatures
Industrial Applications
  • Hydrocarbon cracking
  • Industrial furnace and boiler components and equipment
  • Equipment for Heat-Treating
  • Pressure vessels and heat exchangers
  • Chemical and Petrochemical processing
Material Standards
Rod, Bar, Wire, Forgings, and Forging Stock
ASTM B 408 & ASME SB 408, ASTM B 564 & ASME SB 564, ASME Code Case 1325, ASME Code Case 1949, ISO 9723, ISO 9724, ISO 9725, BS 3076NA15, BS 3075NA15, SEW 470, VdTÜV 412 & 434, DIN 17460, EN 10095
Plate, Sheet, and Strip
ASTM A 240/A 480, ASME SA 240/SA 480, ASTM B 409/B 906, ASME SB 409/SB 906, ASME Code Case 1325, ASME Code Case 2339, BS 3072NA15, BS 3073NA15, SEW 470, VdTÜV 412 & 434, DIN 17460, EN 10028-7 & EN 10095
Pipe & Tube
ASTM B 163, ASME SB 163, ASTM B 407/B 829, ASME SB 407/SB 829, ASTM B 514/B 775, ASME SB 514/SB 775, ASTM B 515/B 751, ASME SB 515/SB 751, ASME Code Case 1325 and 1983, BS 3074NA15, SEW 470, VdTÜV 412 & 434, ISO 6207, DIN 17459
Fittings
ASTM B 366, ASME SB 366
Product Images
Incoloy 800HT Plate close-up showing material texture and surface finish Incoloy 800HT Plate inventory showing various sizes and thicknesses Incoloy 800HT Plate manufacturing process and quality control Incoloy 800HT Plate applications in industrial equipment

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Exporter

  • Total Annual:

    >1000000

  • Employee Number:

    >100

  • Ecer Certification:

    Verified Supplier

Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative... Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative...

+ Read More

Get in touch with us

  • Reach Us
  • JIANGSU MITTEL STEEL INDUSTRIAL LIMITED
  • No.283-1, Youyi Middle Road, Xishan District, Wuxi City, Jiangsu Province
  • https://www.stainless-strips.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement