| Material Grade | Incoloy 800 HT |
| Shape | Flat |
| Technique | Hot Rolled |
| Surface Treatment | Polished |
| Thickness Range | 0.3mm to 120mm |
| Width Range | 1000mm to 2000mm |
| Length Range | 1000mm to 6000mm |
| Iron Content | 39.5% min |
| Nickel Content | 30-35% |
| Chromium Content | 19-23% |
| Aluminum + Titanium | 0.85-1.20% |
| Carbon Content | 0.06-0.10% |
| Max Temperature | 1100°F (600°C) |
| Production Capacity | 500000kgs |
| Edge Type | Mill edge and slit edge |
| Certification | AISI, ASTM |
View Detail Information
Explore similar products
201 304 316L Anti Slip Checkered Stainless Steel Sheet
UNS S32205 Stainless Steel Duplex Plate 2205 Thickness 0.4-16.0mm TISCO POSCO
316L 1.4404 Stainless Steel Plate 3.0-16.0mm Width 1500mm TISCO POSCO
EN 10204-3.1 316L Stainless Plate 1.4404 Hot Rolled 3.0-16.0mm
Product Specification
| Material Grade | Incoloy 800 HT | Shape | Flat |
| Technique | Hot Rolled | Surface Treatment | Polished |
| Thickness Range | 0.3mm to 120mm | Width Range | 1000mm to 2000mm |
| Length Range | 1000mm to 6000mm | Iron Content | 39.5% min |
| Nickel Content | 30-35% | Chromium Content | 19-23% |
| Aluminum + Titanium | 0.85-1.20% | Carbon Content | 0.06-0.10% |
| Max Temperature | 1100°F (600°C) | Production Capacity | 500000kgs |
| Edge Type | Mill edge and slit edge | Certification | AISI, ASTM |
| High Light | Hot Rolled Incoloy 800 HT Plate ,6mm Thick Nickel-Iron-Chromium Alloy Plate ,1500mm Width Superalloy Plate | ||
| Technique | Hot Rolled and Cold Rolled |
|---|---|
| Type | Plate, Coil, Strip |
| Thickness | Hot rolled: 0.3mm to 3mm Cold rolled: 3mm to 120mm |
| Width | 1000mm, 1500mm, 2000mm or customized |
| Length | 1000mm to 6000mm or customized |
| Standard | ASTM A240, ASTM A167, JIS, SUS, EN, DIN, GB, etc |
| Edge | Mill edge and slit edge |
| Material Grade | Monel 400, Monel K-500, Monel R405 |
| MOQ | 1 Ton per specification |
|---|---|
| Incoterm | EXW, FOB, CIF, CFR |
| Loading Port | Shanghai Port |
| Shipping | FCL, LCL, Bulk Ship, Express |
| Delivery | 7-10 days for stock, 15-20 days for production |
| Capacity | 500 tons per year |
| Element | Composition |
|---|---|
| Fe | 39.5% min |
| Ni | 30-35% |
| Cr | 19-23% |
| Al+Ti | 0.85-1.20% |
| C | 0.06-0.10% |
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Exporter
Total Annual:
>1000000
Employee Number:
>100
Ecer Certification:
Verified Supplier
Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative... Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative...
Get in touch with us
Leave a Message, we will call you back quickly!