China S32750 2507 Super Duplex Steel Pipe with Corrosion Resistance High Tensile
China S32750 2507 Super Duplex Steel Pipe with Corrosion Resistance High Tensile

  1. China S32750 2507 Super Duplex Steel Pipe with Corrosion Resistance High Tensile

S32750 2507 Super Duplex Steel Pipe with Corrosion Resistance High Tensile

  1. MOQ: 50 kg
  2. Price: US $6.85-8.5 / kg
  3. Get Latest Price
Model NO. S32750 2507 1.4410
Shape Round
Technique Cold Rolled
Surface Treatment Polished
Outer Diameter 10.3mm - 1219mm
Wall Thickness 1.24mm - 54.59mm
Length as per customer's requirement
Carbon Content 0.03 max
Silicon Content 0.8 max
Manganese Content 1.2 max
Phosphorus Content 0.03 max
Sulfur Content 0.015 max
Chromium Content 24.0-26.0
Nickel Content 6.0-8.0
Molybdenum Content 3.0-5.0

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Model NO. S32750 2507 1.4410 Shape Round
Technique Cold Rolled Surface Treatment Polished
Outer Diameter 10.3mm - 1219mm Wall Thickness 1.24mm - 54.59mm
Length as per customer's requirement Carbon Content 0.03 max
Silicon Content 0.8 max Manganese Content 1.2 max
Phosphorus Content 0.03 max Sulfur Content 0.015 max
Chromium Content 24.0-26.0 Nickel Content 6.0-8.0
Molybdenum Content 3.0-5.0
High Light Corrosion Resistant Super Duplex Steel Pipe ,High Tensile Strength Duplex Stainless Steel Pipe ,Stress Corrosion Cracking Resistance S32750 2507 Pipe
S32750 2507 1.4410 Super Duplex Steel Pipe
Duplex stainless steel was developed to combat common corrosion problems encountered with 300 series stainless steels. The "duplex" structure combines favorable qualities of ferritic alloys (stress corrosion cracking resistance and high strength) with those of austenitic alloys (ease of fabrication and corrosion resistance).
UNS S32750 super duplex stainless steel pipes offer improved corrosion resistance compared to other materials, with greater tensile and yield strength, good ductility, and excellent stress corrosion cracking resistance. These pipes help clients reduce purchase costs while maintaining quality.
Product Specifications
Material Grade S32205, S31803, S32304, S32750, F51, F53, 2205, 2507
Outer Diameter 10.3mm - 1219mm
Wall Thickness 1.24mm - 54.59mm
Length As per customer's requirement
Standard ASTM A789; ASTM A790; EN 10216-5
Applications
  • Petroleum industry
  • Chemical industry
  • Instrumentation
  • Industrial transportation
  • Mechanical structure industry
  • High corrosion resistance applications (offshore industry)
Chemical Composition
Grade C Si Mn P S Cr Ni Mo N
UNS S32750 0.03 max 0.8 max 1.2 max 0.03 max 0.015 max 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32
UNS S31803 0.03 max 1 max 2 max 0.02 max 0.02 max 21.0-23.0 4.5-6.5 2.5-3.5 0.08-0.20
Physical Properties
Grade Y.S. MPa min T.S. Mpa min Elongation % Hardness HRC
UNS S32750 550 800 15 20
UNS S31803 450 620 25 20
Product Advantages
  • Superior surface finish
  • Better mechanical properties
  • More precise dimensions
  • Perfect inspection methods and equipment
Commercial Terms
Price Item FOB, CFR, CIF or as negotiation
Payment T/T, LC or as negotiation
Delivery Time 30 working days after receiving deposit (according to order quantity)
Package Iron case; woven bag or as per customer's requirement
Quality Documentation Mill Test Certificate supplied with shipment, Third Party Inspection acceptable
Quality Testing
  • NDT (Ultrasonic test, Eddy Current test)
  • Mechanical Test (Tension Test, Flaring Test, Flattening Test, Hardness Test, Hydraulic test)
  • Metal Test (Metallographic Analysis, Impact Test - High/low temperature)
  • Chemical Analysis (Photoelectric Emission Spectroscopic)
Main Markets
Europe, Middle East, Southeast Asia, South America
Product Packaging
Super duplex steel pipe packaging - iron case protection Super duplex steel pipe packaging - woven bag protection Super duplex steel pipe packaging - secure industrial packaging

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Exporter

  • Total Annual:

    >1000000

  • Employee Number:

    >100

  • Ecer Certification:

    Verified Supplier

Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative... Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative...

+ Read More

Get in touch with us

  • Reach Us
  • JIANGSU MITTEL STEEL INDUSTRIAL LIMITED
  • No.283-1, Youyi Middle Road, Xishan District, Wuxi City, Jiangsu Province
  • https://www.stainless-strips.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement