| Model NO. | 654smo |
| Shape | Flat |
| Technique | Hot Rolled |
| Surface Treatment | Bright |
| Specification | OD 6-630mm |
| Production Capacity | 50000kgs |
| Material | S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8 |
| Carbon Content | ≤0.02 |
| Silicon Content | ≤0.05 |
| Manganese Content | 2.00-4.00 |
| Nickel Content | 21.0-23.0 |
| Chromium Content | 23-25 |
| Molybdenum Content | 7.0-8.0 |
| Nitrogen Content | 0.45-0.55 |
| Copper Content | 0.3-0.6 |
| Certification | ISO, AISI, ASTM |
View Detail Information
Explore similar products
ASTM A312 309S SS Pipe DIN 1.4833 Seamless Stainless Steel Round Pipe
Grade 310S Stainless Steel Pipe 1.4845 06Cr25Ni20 Heat Resistant
410S Stainless Steel Welded Pipe DN20-DN200 For Ship Structure
EN 10216-5 1.4404 Stainless Steel Pipe Seamless For Pressure Equipment
Product Specification
| Model NO. | 654smo | Shape | Flat |
| Technique | Hot Rolled | Surface Treatment | Bright |
| Specification | OD 6-630mm | Production Capacity | 50000kgs |
| Material | S32652 UNS 654SMO 1.4652 X1CrNiMOCUN24-22-8 | Carbon Content | ≤0.02 |
| Silicon Content | ≤0.05 | Manganese Content | 2.00-4.00 |
| Nickel Content | 21.0-23.0 | Chromium Content | 23-25 |
| Molybdenum Content | 7.0-8.0 | Nitrogen Content | 0.45-0.55 |
| Copper Content | 0.3-0.6 | Certification | ISO, AISI, ASTM |
| High Light | Corrosion Resistant 654smo Seamless Tubing ,High Molybdenum Content Super Austenitic Stainless Steel Pipe ,Excellent Pitting Corrosion Resistance UNS S32654 Seamless Pipe | ||
| Element | Content (%) |
|---|---|
| C | ≤0.02 |
| Si | ≤0.05 |
| Mn | 2.00-4.00 |
| Ni | 21.0-23.0 |
| P | ≤0.03 |
| S | ≤0.005 |
| Cr | 23-25 |
| Mo | 7.0-8.0 |
| N | 0.45-0.55 |
| Cu | 0.3-0.6 |
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Exporter
Total Annual:
>1000000
Employee Number:
>100
Ecer Certification:
Verified Supplier
Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative... Our company is located in Wuxi City, China, we are a stainless steel plate, seamless steel pipe, round steel, steel belt, decorative pipe and other products distribution wholesale private enterprise. Our company operates stainless steel plate, seamless steel pipe, round steel, steel belt, decorative...
Get in touch with us
Leave a Message, we will call you back quickly!