China ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High
China ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High

  1. China ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High
  2. China ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High
  3. China ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High
  4. China ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High

ASTM A790 UNS S32750 Austenitic Stainless Super Duplex Steel Pipe for High

  1. MOQ: 500KGS
  2. Price: Negotiable
  3. Get Latest Price
Payment Terms L/C,T/T
Supply Ability 1500 tons per month
Delivery Time 15-30days
Packaging Details Plywooden Case /Iron Case
Standard ASTM A790
​​Material​ UNS S32750 Super Duplex
Equivalent Standard​ EN 10216-5 / NORSOK M-630
Size Range​ OD: 1/2"~24"
Application Oil and Gas
Type Seamless, Welded
Brand Name YUHONG
Model Number ASTM A790 UNS S32750
Certification ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008
Place of Origin CHINA

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,T/T Supply Ability 1500 tons per month
Delivery Time 15-30days Packaging Details Plywooden Case /Iron Case
Standard ASTM A790 ​​Material​ UNS S32750 Super Duplex
Equivalent Standard​ EN 10216-5 / NORSOK M-630 Size Range​ OD: 1/2"~24"
Application Oil and Gas Type Seamless, Welded
Brand Name YUHONG Model Number ASTM A790 UNS S32750
Certification ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008 Place of Origin CHINA
High Light ASTM A790 super duplex steel pipe ,UNS S32750 seamless stainless pipe ,oil and gas duplex steel pipe

ASTM A790 UNS S32750 Seamless Austenitic Stainless Super Duplex Steel Pipe for Oil and Gas Applications

 

YUHONG GROUP​​ is a leading manufacturer of high-performance stainless steel and duplex pipes, with over 30 years of expertise in serving the global oil & gas industry. Our ​​ASTM A790 UNS S32750 Seamless Super Duplex Steel Pipes​​ are engineered for the most demanding subsea and sour service applications.


Heat Treatment Specifications for S32750

 

Parameter​​ ​​Requirement​​
​​UNS Designation​​ S32750
​​Type​​ 2507
​​Heat Treatment Temperature​​ 1880–2060°F (1025–1125°C)
​​Quenching Method​​ Rapid cooling in air or water
​​Material Standard​​ ASTM A270/A270M (as referenced in the original table)

Chemical Composition of UNS S32750

 

​​Element​​ ​​Requirement (%)​​
Carbon (C), max 0.03
Manganese (Mn), max 1.2
Phosphorus (P), max 0.035
Sulfur (S), max 0.02
Silicon (Si), max 0.8
Nickel (Ni) 6.0–8.0
Chromium (Cr) 24.0–26.0
Molybdenum (Mo) 3.0–5.0
Nitrogen (N) 0.24–0.32
Copper (Cu), max 0.5
Tungsten (W) 0.50–1.00

Mechanical Properties of UNS S32750 

 

Property​​ ​​Requirement​​
​​UNS Designation​​ S32750
​​Type​​ 2507
​​Tensile Strength, min​​ 116 ksi [800 MPa]
​​Yield Strength, min​​ 80 ksi [550 MPa]
​​Elongation, min​​ 15%
​​Hardness, max (HBW)​​ 300
​​Hardness, max (HRC)​​ 32

Advantages of S32750 in Oil & Gas Applications​

  • ​​1.Exceptional Strength for High-Pressure Environments​​
  • ​​2.Superior Resistance to Stress Corrosion Cracking (SCC)​​
  • 3.​​Outstanding Wear and Erosion Resistance​​
  • 4.​​Balanced Ductility for Fabrication​​​
  • 5.​​Cost-Effective Alternative to Nickel Alloys​​
  • 6.​​Performance in Sour Service​​
  • ​​7.Temperature Versatility​​

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Importer,Exporter,Trading Company,Seller,Other

  • Year Established:

    2007

  • Total Annual:

    50M-70M

  • Employee Number:

    50~850

  • Ecer Certification:

    Verified Supplier

  Yuhong Group is one of the large scale group company in China, more than 35 years experience in the international market, providing high-quality services to over 3000 customers, end user which like Aramco, Petrobras, Pemex, Petronas, Ecopetro, Petroecuador, …. till now Yuhong Grou...   Yuhong Group is one of the large scale group company in China, more than 35 years experience in the international market, providing high-quality services to over 3000 customers, end user which like Aramco, Petrobras, Pemex, Petronas, Ecopetro, Petroecuador, …. till now Yuhong Grou...

+ Read More

Get in touch with us

  • Reach Us
  • Yuhong Group Co.,Ltd
  • 20TH FLOOR,NO.1 NEW WORLD BUILDING ,NO.1018 MINAN ROAD,YINZHOU DISTRICT, NINGBO CITY, ZHEJIANG PROVINCE, CHINA
  • https://www.steelseamlesspipe.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement