China Nickel Alloy Steel Inconel 718 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718
China Nickel Alloy Steel Inconel 718 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718

  1. China Nickel Alloy Steel Inconel 718 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718
  2. China Nickel Alloy Steel Inconel 718 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718

Nickel Alloy Steel Inconel 718 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718

  1. MOQ: 1000KGS
  2. Price: USD Negotiable
  3. Get Latest Price
Payment Terms T/T
Supply Ability 200 TONS per month
Delivery Time 7-15 days
Packaging Details Standard export packaging
TYPE OF MATERIAL Nickel-based alloy steel
PRODUCT Inconel 718 ( W.Nr.2.4668 ) Superalloy Seamless Tube
STANDARD ASTM B407, ASTM B515 or as appropriate
GRADE Inconel 718 / NiCr19Fe19Nb5 / N07718
Manufacturing process The steel melt shall be refined with AOD or equivalent.
Surface Finish Solid solution + acid white
Application areas Steam turbine, liquid fuel rocket, low temperature engineering, acid environment, nuclear engineering.
testing facility Accept third party testing such as SGS
Brand Name ABOOM
Model Number Inconel 718
Certification EN 10204 Type 3.1
Place of Origin CHINA

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 200 TONS per month
Delivery Time 7-15 days Packaging Details Standard export packaging
TYPE OF MATERIAL Nickel-based alloy steel PRODUCT Inconel 718 ( W.Nr.2.4668 ) Superalloy Seamless Tube
STANDARD ASTM B407, ASTM B515 or as appropriate GRADE Inconel 718 / NiCr19Fe19Nb5 / N07718
Manufacturing process The steel melt shall be refined with AOD or equivalent. Surface Finish Solid solution + acid white
Application areas Steam turbine, liquid fuel rocket, low temperature engineering, acid environment, nuclear engineering. testing facility Accept third party testing such as SGS
Brand Name ABOOM Model Number Inconel 718
Certification EN 10204 Type 3.1 Place of Origin CHINA
High Light inconel metal ,inconel steel

Nickel Alloy Steel Inconel 718 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718

 

Inconel 718 W.Nr.2.4668 Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718

 

Inconel 718 ( W.Nr.2.4668 ) Superalloy Seamless Tube NiCr19Fe19Nb5 / N07718

 

Material designation: Inconel 718 nickel based alloy
US grade: N07718
German grade: W.Nr.2.4668 / NiCr19Fe19Nb5
French grade: Nc19FeNb

 


Overview of Inconel 718 (N07718) nickel-based alloy:

 

The chemical composition of this alloy is divided into 3 categories: standard composition, high-quality composition, and high-purity composition, see Table 1-1. The high-quality ingredients reduce carbon and increase niobium on the basis of standard ingredients, thereby reducing the amount of niobium carbide, reducing fatigue sources and increasing the number of strengthening phases, and improving fatigue resistance and material strength. At the same time reduce harmful impurities and gas content. High-purity ingredients reduce the content of sulfur and harmful impurities on the basis of high-quality standards, and improve the purity and comprehensive performance of materials.
Inconel718 alloy for nuclear energy applications needs to control the boron content (the other element composition is unchanged), and the specific content is determined by the supplier and the buyer through consultation. When ω (B) ≤ 0.002%, it is distinguished from the Inconel718 alloy used in the aerospace industry, and the alloy grade is Inconel718A.

 

Table1-1                                                                                    %

type C Cr Ni Co Mo Al Ti Fe
normal ≤0.08 17.0~21.0 50.0~55.0 ≤1.0 2.80~3.30 0.30~0.70 0.75~1.15 Balance
high- grade 0.02~0.06 17.0~21.0 50.0~55.0 ≤1.0 2.80~3.30 0.30~0.70 0.75~1.15 Balance
High- purity 0.02~0.06 17.0~21.0 50.0~55.0 ≤1.0 2.80~3.30 0.30~0.70 0.75~1.15 Balance
type Nb B Mg Mn Si P S Cu Ca
≤
normal 4.75~5.50 0.006 0.01 0.35 0.35 0.015 0.015 0.30 0.01
high- grade 5.00~5.50 0.006 0.01 0.35 0.35 0.015 0.015 0.30 0.01
High- purity 5.00~5.50 0.006 0.005 0.35 0.35 0.015 0.002 0.30 0.005

 

type Bi Sn Pb Ag Se Te Tl N O
≤  
normal --- --- 0.0005 --- 0.0003 --- --- --- ---
high- grade 0.001 0.005 0.001 0.001 0.0003 --- --- 0.01 0.01
High- purity 0.00003 0.005 0.001 0.001 0.0003 0.00005 0.0001 0.01 0.005

 

specification:


Outer diameter Φ6—630mm; wall thickness: 1-50mm, maximum length 18000mm
Special specifications are available upon negotiation.

 

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Employee Number:

    >100

  • Ecer Certification:

    Active Member

                      Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...                       Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...

+ Read More

Get in touch with us

  • Reach Us
  • Shanghai Aboom Metal prodcut co.,ltd
  • NO.161 XingFei Road ,Songjiang Disrict,Shanghai 201601, P.R.CHINA
  • http://www.superduplexss.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement