| TYPE OF MATERIAL | nickel based alloy |
| PRODUCT | Inconel 601 UNS N06601 nickel based alloy seamless pipe |
| STANDARD | ASTM SB167 |
| GRADE | Inconel 601 / UNS N06601 / 2.4851 |
| Manufacturing process | The steel melt shall be refined with AOD or equivalent. |
| Heat Treatment | shall be supplied in the solution annealed / water quenched condition. |
| Surface Finish | Descaled, White Pickled, and Passivated Condition |
| testing facility | Accept third party testing such as SGS |
| Brand Name | ABOOM |
| Model Number | Inconel 601 |
| Certification | EN 10204 Type 3.1 |
| Place of Origin | CHINA |
View Detail Information
Explore similar products
ASTM SB167 Nickel Based 2.4816 Inconel Alloy
Nickel Based Anti Oxidation UNS N06600 Inconel 600 Plate
Anti Oxidation ASTM A240 UNS N07617 Inconel 617 Plate
N06625 Inconel Alloy Inconel 625 Sheet Plate Stock Nickel Based Alloy
Product Specification
| Payment Terms | T/T | Supply Ability | 200 TONS PER MONTH |
| Delivery Time | 7-15dyas | Packaging Details | Standard export packaging |
| TYPE OF MATERIAL | nickel based alloy | PRODUCT | Inconel 601 UNS N06601 nickel based alloy seamless pipe |
| STANDARD | ASTM SB167 | GRADE | Inconel 601 / UNS N06601 / 2.4851 |
| Manufacturing process | The steel melt shall be refined with AOD or equivalent. | Heat Treatment | shall be supplied in the solution annealed / water quenched condition. |
| Surface Finish | Descaled, White Pickled, and Passivated Condition | testing facility | Accept third party testing such as SGS |
| Brand Name | ABOOM | Model Number | Inconel 601 |
| Certification | EN 10204 Type 3.1 | Place of Origin | CHINA |
| High Light | inconel metal ,inconel steel | ||
2.4851 Inconel Alloy Inconel 601 Pipe UNS N06601 Nickel Based Superalloys
Inconel 601 UNS N06601 nickel based alloy seamless pipe 2.4851
Material designation: Inconel 601 nickel based alloy
US grade: N06601
German grade: 2.4851
Inconel 601 (N06601) nickel-based alloy processing heat treatment:
Inconel 601 (UNS N06601) nickel-based alloy is not a precipitation hardening alloy, so it cannot be aged hardened by heat treatment. When the temperature after cold working reaches about 900 ° C, the material softens. If the material needs high-temperature strength, it is recommended that the solution heat treatment be performed at a temperature of 1100 to 1200 ° C. At this time, the cooling method is water cooling.
Depending on the thickness of the plate, air cooling can also be used. However, in order to avoid carbide precipitation, it is recommended to cool as quickly as possible in the temperature range of 500 to 800 ° C.
Inconel 601 (N06601) nickel-based alloy chemical composition: see Table-1:
Table-1 %
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.10 | 0.50 | 1.00 | 0.020 | 0.015 | 21.0-25.0 | 72.0 | 1.00 | |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | Co≤ | V≤ | W≤ | Nb≤ |
| 1.00-1.70 | Balance |
specification:
Outer diameter Φ6—762mm; wall thickness: 0.5-50mm, maximum length 18000mm
Special specifications are available upon negotiation.
![]()
Company Details
Business Type:
Manufacturer
Employee Number:
>100
Ecer Certification:
Active Member
Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio... Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...
Get in touch with us
Leave a Message, we will call you back quickly!