| Payment Terms | L/C, T/T, Western Union, Paypal |
| Supply Ability | 50 sets per month |
| Delivery Time | 30 work days |
| Packaging Details | wood carton |
| Product Name | Ultrasonic Rotary Edge Welding Machine |
| Voltage | AC220V/380V |
| Power | 4200W |
| Welding Area | OD 5 mm~ 150 mm |
| OEM/ODM | Available |
| Plastic Processed | Thermo plastic PPO/PP/PSO/PS/PPS/PET/PE/PC |
| Usage | Plastic Welding |
| After-sales Service Provided | Free spare parts, commissioning and training,Online support,Video technical support |
| Brand Name | KnMTech |
| Model Number | KM-QD-1542R |
| Place of Origin | China |
View Detail Information
Explore similar products
Non Woven Face Mask Edge Welding 20KHz 2KW Ultrasonic Sealing Machine
Digital Ultrasonic Welding Machine Auto Tuning Frequency 15KHz 3200W
15kHz 2600W Standard Good Stability Ultrasonic Plastic Welding Machine
15khz 2200W Economical Type Plastic Ultrasonic Welding Press for PP ABS
Product Specification
| Payment Terms | L/C, T/T, Western Union, Paypal | Supply Ability | 50 sets per month |
| Delivery Time | 30 work days | Packaging Details | wood carton |
| Product Name | Ultrasonic Rotary Edge Welding Machine | Voltage | AC220V/380V |
| Power | 4200W | Welding Area | OD 5 mm~ 150 mm |
| OEM/ODM | Available | Plastic Processed | Thermo plastic PPO/PP/PSO/PS/PPS/PET/PE/PC |
| Usage | Plastic Welding | After-sales Service Provided | Free spare parts, commissioning and training,Online support,Video technical support |
| Brand Name | KnMTech | Model Number | KM-QD-1542R |
| Place of Origin | China | ||
| High Light | 6 Station Ultrasonic Rotary Welding Machine ,150mm Ultrasonic Rotary Welding Machine ,PPO Ultrasonic Rotary Welding Machine | ||
6-Station Ultrasonic Rotary Welding Machine for Plastic Welding
Technical parameters:
| Place of Origin: | Jiangsu, China (Mainland) | Brand Name: | KnMTECH |
| Origin: | China | Weight: | 290 kg / 320 kg |
| Voltage: | AC220V/380V | Power: | 4200W |
| Frequency: | 15KHZ | Welding Area: | OD 5 mm~ 150 mm |
| Dimensions: | L900*W780*H2000mm | Usage: | Plastic Welding |
| After-sales Service Provided: | Free spare parts, commissioning and training, Online support, Video technical support | Warranty: | 1 Year |
| Application: | Plastics/electrics/auto/package/environmental /medical /cloth/toy | Packaging: | Wooden Case Packaging |
| Plastic Processed: | Thermoplastic PPO/PP/PSO/PS/PPS/PET/PE/PC | OEM/ODM: | Available |
This ultrasonic rotary welding machine is customized with 6 stations on the Index plate. The ultrasonic rotary edge welding machine can be used for welding thermoplastics, Such as plastic toys, plastic gifts, household plastic electronic appliances, packing bags, etc.
Main Functions:
1. According to the product requirements, drive mode can be pneumatic, hydraulic, or servo motor drive.
2. The welding temperature, heating time, cooling time, welding depth, pressure, transit time are adjustable parameters.
3. Semi-automatic or fully automatic mode will be designed as per the products to be welded.
Features:
* high efficiency
* no distortion
* no pollution, environmentally friendly
* welding firmly
Applications:
| Application Industry | Application Products |
| Consumer Products | daily necessities, stationery, filter, folder and shell, pen stand, cosmetics box shell, the end of the toothpaste tube seal, mirror, insulated cup, lighter. |
| Electronics | recording, audiotape boxes and core wheel, disk enclosure, the board of mobile phone batteries and rectifier transformers, switches and sockets, remote control, |
| Home appliances | Balance ring, electronic clock, electric trumpeter hairdryer, steam iron water tank |
| Toy | plastic toys, water guns, aquatic life video game, children dolls, plastic gifts, etc |
| Film & Fabric | Filters, Shower Curtains, Biodegradable Bag, Non-Woven Face Mark,..etc. |
| Medical | Surgical Instruments,Testing Equipment,filters,I-V units,insulated |
FAQ:
1. How long is your warranty for the ultrasonic welding machine?
One year Warranty with none human damage.
In this period factory, will responsible for repair fix it for free or the factory will send the new parts to the customer instead of the broken parts for free. After warranty time, the factory will repair fix it or send the new parts at the cost price.
2. Can we agent your ultrasonic welding machines in our country or city?
Of course. We are looking for a sole agent in the country who has the willingness to cooperate with us for a long business term.
3. could you make it according to our special requirements?
Of course, we can do that. Please tell us your idea or your application.
Detailed Photos:
![]()
![]()
![]()
Company Details
Business Type:
Exporter
Year Established:
2009
Ecer Certification:
Active Member
Incorporated in 2015, K& M Technologies Ltd is one-stop solution provider in plastic welding business, especially in ultrasonic plastic welding, ultrasonic non-woven fabric sealing and cutting, hot plate welding, water filter welding lines... From June 2021, We started the cooperation with a ... Incorporated in 2015, K& M Technologies Ltd is one-stop solution provider in plastic welding business, especially in ultrasonic plastic welding, ultrasonic non-woven fabric sealing and cutting, hot plate welding, water filter welding lines... From June 2021, We started the cooperation with a ...
Get in touch with us
Leave a Message, we will call you back quickly!