China AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace
China AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace

  1. China AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace
  2. China AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace
  3. China AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace

AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace

  1. MOQ: 30 Kg
  2. Price: Negotiable
  3. Get Latest Price
Payment Terms L/C, T/T, Western Union, MoneyGram
Supply Ability 300 tons per month
Delivery Time 20~40 Days
Packaging Details Spool Carton box, Coil package with polybag,then in woodencase
Name AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components
Material Nickel Chromium Iron
Ni (Min) 50~55%
Density 8.24 g/cm3
Melting point 1260-1320°C
Elongation (≥ %) 25 %
Thermal conductivity 15.9 W/m·K
Finishing Bright,Oxided, acid white
Application Construction, Industry Oil, piping systems
Yield strength 550MPa
Tensile strength 910 MPa
Hardness ≤ 363 HB
Standard ASTM, ASME
size 6~200mm
shape Round, Square, flat
Brand Name Victory
Model Number Inconel 718
Certification ISO9001 ROHS
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C, T/T, Western Union, MoneyGram Supply Ability 300 tons per month
Delivery Time 20~40 Days Packaging Details Spool Carton box, Coil package with polybag,then in woodencase
Name AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components Material Nickel Chromium Iron
Ni (Min) 50~55% Density 8.24 g/cm3
Melting point 1260-1320°C Elongation (≥ %) 25 %
Thermal conductivity 15.9 W/m·K Finishing Bright,Oxided, acid white
Application Construction, Industry Oil, piping systems Yield strength 550MPa
Tensile strength 910 MPa Hardness ≤ 363 HB
Standard ASTM, ASME size 6~200mm
shape Round, Square, flat Brand Name Victory
Model Number Inconel 718 Certification ISO9001 ROHS
Place of Origin China
High Light Aerospace Components Inconel 718 StripASTM B670 Inconel 718 StripAMS 5596 Inconel 718 Strip

Advantages of Inconel 718 Strips



High Strength-to-Weight Ratio: Provides durability without adding excessive weight.
Excellent Fabricability: Can be easily machined and formed into complex shapes.
Resistance to Oxidation and Corrosion: Ensures longevity in challenging environments.

 

 

Applications of Inconel 718 Strips


Aerospace Components

Thrust Reversers: Used in thrust reversers for jet engines, where high-temperature resistance and strength are essential.
Structural Components: Fabricated into various structural parts that require lightweight yet strong materials.
Oil and Gas Industry

Downhole Equipment: Employed in valves, fittings, and other components exposed to harsh environments.
Subsea Applications: Ideal for use in subsea pipelines and connectors due to its excellent corrosion resistance.
Nuclear Applications

Fuel Rods and Structural Supports: Used in nuclear reactors where materials must withstand extreme conditions.
Marine Applications

Components in Marine Engines: Suitable for various parts exposed to seawater, where corrosion resistance is vital.
High-Performance Engineering

Fasteners and Bolts: Can be used to manufacture bolts and fasteners that require superior mechanical properties.
Heat Exchangers

Heat Exchanger Tubes: Utilized in heat exchangers where high temperatures and corrosive fluids are present.

 

 

Parameter:

Chemical Properties of Inconel 718

 

Nickel (plus Cobalt) .......................................................50.00-55.00

Chromium......................................................................17.00-21.00

Iron .....................................................................................Balance

Niobium (plus Tantalum)....................................................4.75-5.50

Molybdenum .....................................................................2.80-3.30

Titanium.............................................................................0.65-1.15

Aluminum ..........................................................................0.20-0.80

Cobalt ...............................................................................1.00 max.

Carbon..............................................................................0.08 max.

Manganese .......................................................................0.35 max.

Silicon ...............................................................................0.35 max.

Phosphorus.....................................................................0.015 max.

Sulfur...............................................................................0.015 max.

Boron ..............................................................................0.006 max.

Copper..............................................................................0.30 max

 

 

Density 8.19g/cm³ 0.296 lb/in³
Melting point 1260-1336 2437°F

 

SPECIFICATIONS
 
Form
  ASTM
Rod,bar and wire
B 166
Plate,sheet and strip
B 168, B 906
Seamless pipe and tube
B 167, B 829
Welded pipe
B 517, B775
Fitting 
B 366
Billet and bar for reforging
B 472
Forging
B 564

 

Inconel series

Steel grade
Inconel 600
Inconel 601
Inconel 625
Inconel 718
Inconel 725
Inconel X-750
Corresponding brand
N06600/2.4816/1Cr15Ni75Fe8/NS312/CY40
N06601/2.4851/1Cr23Ni60Fe13AI/NS313
N06625/2.4856/0Cr20Ni65Mo10bN4/NS336
N07718/2.4668/GH4169
N07725
N07750/2.4669/GH4145
Chemical composition%
C≤
0.150
0.100
0.100
0.080
0.030
0.080
Mn≤
1.00
1.00
0.50
0.35
0.35
1.00
P≤
/
/
0.015
0.015
0.015
/
S≤
0.015
0.015
0.015
0.015
0.010
0.010
Si≤
0.50
0.50
0.50
0.35
0.20
0.50
Cr≤
14.0-17.0
21.0-25.0
20.0-23.0
17.0-21.0
19.0-22.5
14.0-17.0
Ni≤
≥72.0
58.0-63.0
≥58.0
55.0-59.0
55.0-59.0
≥70
Mo
/
/
8.0-10.0
2.8-3.3
7.0-9.5
/
Cu
≤0.50
≤1.50
/
≤0.30
/
≤0.50
N
/
/
/
 
/
/
Nb
/
/
3.15-4.15
4.75-5.50
2.75-4.00
0.70-1.20
other
Fe:6.0-10.0
Al:1.0-1.7
Co:≤1.0Ai:≤0.40Tr:0.40Fe:≤5.0
AI:0.20-0.80Ti:0.65-1.15B≤0.006
Tr:1.0-1.7AI≤0.35
Co:≤1.0 AI:0.4-1.0Tr:0.25-2.75Fe:5.0-9.0

 

 

Customize size as below

 

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

 

 

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

 

 

 

 

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Trading Company,Seller

  • Year Established:

    2008

  • Total Annual:

    100-100000

  • Employee Number:

    100~150

  • Ecer Certification:

    Verified Supplier

Changzhou Victory Technology Co., Ltd is a leading manufacturer of high-quality nickel alloy products. We offer a wide range of solutions, including pipes, fittings, bars, sheets, and wires, specializing in grades such as Monel, Inconel, Incoloy, and Hastelloy. With a focus on innovation a... Changzhou Victory Technology Co., Ltd is a leading manufacturer of high-quality nickel alloy products. We offer a wide range of solutions, including pipes, fittings, bars, sheets, and wires, specializing in grades such as Monel, Inconel, Incoloy, and Hastelloy. With a focus on innovation a...

+ Read More

Get in touch with us

  • Reach Us
  • Changzhou Victory Technology Co., Ltd
  • NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
  • https://www.victory-alloy.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement