| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Supply Ability | 300 tons per month |
| Delivery Time | 20~40 Days |
| Packaging Details | Spool Carton box, Coil package with polybag,then in woodencase |
| Name | High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate |
| Material | Nickel Chromium Iron |
| Ni (Min) | 50~55% |
| Density | 8.24 g/cm3 |
| Melting point | 1260-1320°C |
| Elongation (≥ %) | 25 % |
| Thermal conductivity | 15.9 W/m·K |
| Finishing | Bright,Oxided, acid white |
| Application | Construction, Industry Oil, piping systems |
| Yield strength | 550MPa |
| Tensile strength | 910 MPa |
| Hardness | ≤ 363 HB |
| Standard | ASTM, ASME |
| size | 6~200mm |
| shape | Round, Square, flat |
| Brand Name | Victory |
| Model Number | Inconel 718 |
| Certification | ISO9001 ROHS |
| Place of Origin | China |
View Detail Information
Explore similar products
Nickel Alloy UNS N06600 Inconel 600 Wire
Oil And Gas Industry Nickel Based Alloy Wire Inconel 825 Wire With High
Aviation Engine Manufacturing Nickel Base Alloy Inconel 718 Wire With High
Aerospace Inconel 617 Alloy Wire High Temperature Resistance
Product Specification
| Payment Terms | L/C, T/T, Western Union, MoneyGram | Supply Ability | 300 tons per month |
| Delivery Time | 20~40 Days | Packaging Details | Spool Carton box, Coil package with polybag,then in woodencase |
| Name | High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate | Material | Nickel Chromium Iron |
| Ni (Min) | 50~55% | Density | 8.24 g/cm3 |
| Melting point | 1260-1320°C | Elongation (≥ %) | 25 % |
| Thermal conductivity | 15.9 W/m·K | Finishing | Bright,Oxided, acid white |
| Application | Construction, Industry Oil, piping systems | Yield strength | 550MPa |
| Tensile strength | 910 MPa | Hardness | ≤ 363 HB |
| Standard | ASTM, ASME | size | 6~200mm |
| shape | Round, Square, flat | Brand Name | Victory |
| Model Number | Inconel 718 | Certification | ISO9001 ROHS |
| Place of Origin | China | ||
| High Light | High strength Nickel-chromium alloy 718 ,Nickel-chromium alloy 718 strip ,Nickel-chromium alloy 718 foil | ||
Inconel 718 Alloy
Inconel 718 is a precipitation hardened nickel-based alloy designed to display exceptionally high yield, tensile and creep-rupture properties at temperatures up to 1300°F (704°C). The age-hardening response of Inconel 718 permits annealing and welding without spontaneous hardening during heating and cooling. Nickel Alloy 718 has excellent weldability when compared to the nickel-base super alloys hardened by aluminum and titanium.
Advantages of Inconel 718 Strips
Applications of Inconel 718 Strips
Chemical Properties of Inconel 718
Nickel (plus Cobalt) .......................................................50.00-55.00
Chromium......................................................................17.00-21.00
Iron .....................................................................................Balance
Niobium (plus Tantalum)....................................................4.75-5.50
Molybdenum .....................................................................2.80-3.30
Titanium.............................................................................0.65-1.15
Aluminum ..........................................................................0.20-0.80
Cobalt ...............................................................................1.00 max.
Carbon..............................................................................0.08 max.
Manganese .......................................................................0.35 max.
Silicon ...............................................................................0.35 max.
Phosphorus.....................................................................0.015 max.
Sulfur...............................................................................0.015 max.
Boron ..............................................................................0.006 max.
Copper..............................................................................0.30 max
| Density | 8.19g/cm³ | 0.296 lb/in³ |
| Melting point | 1260-1336 | 2437°F |
Inconel series
Customize size as below
| Shape | Size(mm) |
| WIre | 0.5-7.5 |
| Rod/Bar | 8.0-200 |
| Strip | (0.5-2.5)*(5-180) |
| Tube | custom made |
| Plate | custom made |
contact us
email:victory@dlx-alloy.com
Oem service:
Welcome customized size
We are experience factory for OEM&ODM service
![]()
![]()
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Trading Company,Seller
Year Established:
2008
Total Annual:
100-100000
Employee Number:
100~150
Ecer Certification:
Active Member
Changzhou Victory Technology Co., Ltd is a leading manufacturer of high-quality nickel alloy products. We offer a wide range of solutions, including pipes, fittings, bars, sheets, and wires, specializing in grades such as Monel, Inconel, Incoloy, and Hastelloy. With a focus on innovation a... Changzhou Victory Technology Co., Ltd is a leading manufacturer of high-quality nickel alloy products. We offer a wide range of solutions, including pipes, fittings, bars, sheets, and wires, specializing in grades such as Monel, Inconel, Incoloy, and Hastelloy. With a focus on innovation a...