View Detail Information
Explore similar products
Yttria-Stabilized Zirconia (YSZ) Crucibles for Powder Metallurgy | High-Purity
Mg-PSZ Crucibles | Magnesia-Stabilized Zirconia Melting Pots for Vacuum
Custom YSZ Crucibles for Powder Metallurgy | Precision Ceramic Crucibles for
Custom Zirconia Crucibles | 94-99% ZrO₂ | High-Temperature & Extreme Chemical
Product Specification
| High Light | Magnesium-Stabilized Zirconia crucibles ,High-temperature ceramic crucibles for superalloy ,Mg-PSZ crucibles for reactive metal melting | ||
Magnesium-Stabilized Zirconia (Mg-PSZ) crucibles represent a specialized class of advanced ceramic containers engineered for the most extreme high-temperature and chemically aggressive environments. Unlike yttria-stabilized variants, Mg-PSZ crucibles utilize magnesium oxide (MgO) as the stabilizing agent—typically 2.9-3.5%—to maintain the zirconia in a partially stabilized state that delivers exceptional thermal shock resistance and mechanical toughness .
With a distinctive yellow appearance, these crucibles are designed for continuous operation at 2000-2200°C in air, vacuum, or protective atmospheres, making them the preferred choice for melting superalloys, reactive metals, and precious metals where contamination cannot be tolerated .
Key Applications:
Superalloy Melting: Vacuum induction melting (VIM) of nickel, cobalt, and iron-based superalloys
Reactive Metal Processing: Titanium, zirconium, hafnium, and their alloys
Precious Metal Refining: Gold, platinum, palladium, rhodium
Aerospace Alloy Development: High-temperature alloy research and production
Specialty Glass Manufacturing: High-temperature glass compositions
Advanced Material Research: Energy materials, rare earth processing
Company Details
Business Type:
Manufacturer
Year Established:
2020
Total Annual:
>10000000
Employee Number:
150~200
Ecer Certification:
Verified Supplier
Who We Are Hunan Xiaoqing Ceramics Co., Ltd. is a high-tech enterprise dedicated to advanced precision ceramics. Built on robust IATF 16949 and defense-grade quality systems, we have grown within a strong industrial ecosystem and established long-term cooperation with over 40 leading companies wor... Who We Are Hunan Xiaoqing Ceramics Co., Ltd. is a high-tech enterprise dedicated to advanced precision ceramics. Built on robust IATF 16949 and defense-grade quality systems, we have grown within a strong industrial ecosystem and established long-term cooperation with over 40 leading companies wor...