China GH738 Alloy Ni Based Superalloy With High Strength And Oxidation Resistance
China GH738 Alloy Ni Based Superalloy With High Strength And Oxidation Resistance

  1. China GH738 Alloy Ni Based Superalloy With High Strength And Oxidation Resistance
  2. China GH738 Alloy Ni Based Superalloy With High Strength And Oxidation Resistance

GH738 Alloy Ni Based Superalloy With High Strength And Oxidation Resistance

  1. MOQ: 100KG
  2. Price: Price is negotiated based on the required specifications and quantity
  3. Get Latest Price
Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation
Packaging Details Standard export packaging, or packaging as required
Density 8.19 g/cm³
Melting Point 1260-1340°C
Tensile Strength 900-1100 MPa
Yield Strength 700-850 MPa
Elongation 20-35%
Hardness 250-300 HB
Thermal Conductivity 11.2 W/m·K
Oxidation Resistance Excellent
Applications Aerospace, Gas Turbines, High-temp. Components
Brand Name Zhonggong Special Metallurgy
Model Number GH738 Alloy
Place of Origin China
Certification ISO Certificate

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P, Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation Packaging Details Standard export packaging, or packaging as required
Density 8.19 g/cm³ Melting Point 1260-1340°C
Tensile Strength 900-1100 MPa Yield Strength 700-850 MPa
Elongation 20-35% Hardness 250-300 HB
Thermal Conductivity 11.2 W/m·K Oxidation Resistance Excellent
Applications Aerospace, Gas Turbines, High-temp. Components Brand Name Zhonggong Special Metallurgy
Model Number GH738 Alloy Place of Origin China
Certification ISO Certificate
High Light GH738 Ni Based Superalloy ,Ni Based Superalloy High Strength

GH738 Alloy is a high-performance, nickel-based superalloy engineered for exceptional mechanical strength and superior oxidation resistance at elevated temperatures. It is commonly used in aerospace and industrial gas turbine applications due to its ability to maintain structural integrity under extreme conditions.

Key Features:

  • Composition: Primarily nickel, with additions of chromium, cobalt, and other elements for enhanced high-temperature stability and strength.
  • Mechanical Properties: Provides high tensile and yield strength, excellent fatigue resistance, and good ductility.
  • Thermal Stability: Retains mechanical properties over a broad temperature range, making it suitable for high-temperature environments.
  • Oxidation Resistance: Exhibits outstanding resistance to oxidation and corrosion, contributing to longer service life in harsh conditions.
  • Applications: Ideal for components such as turbine blades, vanes, and other critical parts in aerospace engines and industrial turbines.

GH738 Alloy’s robust performance characteristics make it a preferred choice for demanding applications where reliability and durability are paramount.

 

Here’s a table detailing the typical chemical composition of GH738 Alloy:

Element Content (%)
Nickel (Ni) 50.0 - 60.0
Chromium (Cr) 20.0 - 25.0
Cobalt (Co) 7.0 - 10.0
Molybdenum (Mo) 3.0 - 5.0
Titanium (Ti) 2.5 - 4.0
Aluminum (Al) 1.5 - 2.5
Iron (Fe) Balance
Carbon (C) ≤ 0.08
Boron (B) ≤ 0.01
Other Elements Traces

This composition provides GH738 Alloy with its high-temperature strength and resistance to oxidation and corrosion.

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company

  • Year Established:

    2010

  • Total Annual:

    1000000-1500000

  • Employee Number:

    100~200

  • Ecer Certification:

    Active Member

Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507​,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507​,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...

+ Read More

Get in touch with us

  • Reach Us
  • Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
  • New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
  • https://www.zd-1stainless-steelss.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement