China GH32 Alloy Nickel Alloy Rod High Strength Corrosion Resistance Nickel Based
China GH32 Alloy Nickel Alloy Rod High Strength Corrosion Resistance Nickel Based

  1. China GH32 Alloy Nickel Alloy Rod High Strength Corrosion Resistance Nickel Based
  2. China GH32 Alloy Nickel Alloy Rod High Strength Corrosion Resistance Nickel Based

GH32 Alloy Nickel Alloy Rod High Strength Corrosion Resistance Nickel Based

  1. MOQ: 100KG
  2. Price: Price is negotiated based on the required specifications and quantity
  3. Get Latest Price
Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation
Packaging Details Standard export packaging, or packaging as required
Brand Name Zhonggong Special Metallurgy
Model Number GH32 Alloy
Place of Origin China
Certification ISO Certificate

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P, Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation Packaging Details Standard export packaging, or packaging as required
Brand Name Zhonggong Special Metallurgy Model Number GH32 Alloy
Place of Origin China Certification ISO Certificate
High Light GH32 Nickel Alloy Rod ,Nickel Alloy Rod Corrosion Resistance ,GH32 Nickel Based Superalloy

GH32 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. Known for its superior mechanical properties, GH32 offers exceptional strength, excellent oxidation resistance, and outstanding corrosion resistance. The alloy's composition typically includes nickel, chromium, cobalt, molybdenum, and other elements to enhance its durability and stability at elevated temperatures.

Key Features:

  • Composition: Predominantly nickel with chromium, cobalt, and molybdenum, tailored to enhance strength and stability.
  • Temperature Resistance: Effective at temperatures up to approximately 950°C (1742°F), maintaining mechanical integrity and performance.
  • Mechanical Properties: High tensile and yield strength, ensuring reliability in high-stress environments.
  • Oxidation and Corrosion Resistance: Excellent resistance to oxidation and corrosion, suitable for harsh environments.
  • Applications: Ideal for aerospace components, gas turbines, and other critical parts requiring high-temperature stability.
  • Heat Treatment: Capable of being heat-treated to optimize its mechanical properties and overall performance.

GH32 Alloy is utilized in applications where high strength, temperature stability, and resistance to harsh conditions are essential. Its advanced properties ensure reliable performance in some of the most challenging industrial and aerospace environments.

 

Here’s a detailed composition table for GH32 Alloy:

Element Composition (%)
Nickel (Ni) Balance
Chromium (Cr) 19.0 - 21.0
Cobalt (Co) 10.0 - 12.0
Molybdenum (Mo) 2.0 - 4.0
Titanium (Ti) 2.0 - 2.5
Aluminum (Al) 1.0 - 1.5
Carbon (C) ≤ 0.08
Silicon (Si) ≤ 0.50
Manganese (Mn) ≤ 0.50
Boron (B) ≤ 0.01

These values provide a general guideline, but specific alloy grades may have slight variations based on the manufacturer's standards and requirements.

 

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company

  • Year Established:

    2010

  • Total Annual:

    1000000-1500000

  • Employee Number:

    100~200

  • Ecer Certification:

    Active Member

Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507​,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507​,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...

+ Read More

Get in touch with us

  • Reach Us
  • Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
  • New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
  • https://www.zd-1stainless-steelss.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement