| Model NO. | 254SMO |
| Shape | Round |
| Technique | Hot Rolled |
| Surface Treatment | Pickling |
| Length | 6m or Cutting Any Length as Request |
| Diameter | 6 - 406mm |
| Thickness | Sch10 Sch40s Sch160 |
| Specification | DN10 - DN600 |
| Production Capacity | 100000 PCS / Year |
| Wall Thickness | SCH10S - XXS or unstandard size as request |
| Standard | ASTM JIS EN DIN |
| Type | Seamless Pipe / Welded Pipe |
| Nickel Content | 17.5 - 18.5% |
| Chromium Content | 19.5 - 20.5% |
| Molybdenum Content | 6.0 - 6.5% |
| Certification | ISO, ASTM |
View Detail Information
Explore similar products
ASTM A312 TP316L Stainless Steel Seamless Pipe 1.4404 Hollow Bar OD 90 ID 60 MM
Hollow Bar Seamless Sus316L OD45x28ID L3000 Mm ASTM A276 TP316L Stainless Steel
ASTM A790 S32750 2507 DIN1.4410 Super Duplex Steel Seamless Pipe 89*6*6000mm
Super Duplex 2507 Pipe And ASTM A790 S32750 Seamless Stainless Steel Pipe For
Product Specification
| Model NO. | 254SMO | Shape | Round |
| Technique | Hot Rolled | Surface Treatment | Pickling |
| Length | 6m or Cutting Any Length as Request | Diameter | 6 - 406mm |
| Thickness | Sch10 Sch40s Sch160 | Specification | DN10 - DN600 |
| Production Capacity | 100000 PCS / Year | Wall Thickness | SCH10S - XXS or unstandard size as request |
| Standard | ASTM JIS EN DIN | Type | Seamless Pipe / Welded Pipe |
| Nickel Content | 17.5 - 18.5% | Chromium Content | 19.5 - 20.5% |
| Molybdenum Content | 6.0 - 6.5% | Certification | ISO, ASTM |
| High Light | Corrosion Resistant 254SMO Stainless Steel Pipe ,High Molybdenum Content Stainless Steel Pipe ,Seawater Applications UNS S31254 Stainless Tube | ||
254SMO Stainless Steel Pipe Tube UNS S31254 is a super-austenitic stainless steel designed for maximum resistance to pitting and crevice corrosion. With high levels of chromium, molybdenum, and nitrogen, this alloy is especially suited for high chloride environments including brackish water, seawater, pulp mill bleach plants, and other high chloride process streams.
254SMO pipes offer superior chloride resistance compared to Alloy 904L, Alloy 20, Alloy 825, and Alloy G. The copper content improves corrosion resistance in certain acids, while the high nickel, chromium, and molybdenum content provides excellent stress corrosion cracking performance.
| Element | Min (%) | Max (%) |
|---|---|---|
| Nickel (Ni) | 17.5 | 18.5 |
| Chromium (Cr) | 19.5 | 20.5 |
| Molybdenum (Mo) | 6.0 | 6.5 |
| Copper (Cu) | 0.50 | 1.00 |
| Nitrogen (N) | 0.18 | 0.22 |
| Carbon (C) | - | 0.020 |
| Manganese (Mn) | - | 1.00 |
| Silicon (Si) | - | 0.80 |
| Phosphorus (P) | - | 0.03 |
| Sulfur (S) | - | 0.010 |
254SMO features a face-centered cubic lattice structure and is typically annealed at 1150-1200°C to obtain austenitic structure. The material maintains excellent impact strength and corrosion resistance under normal operating conditions.
Company Details
Business Type:
Manufacturer
Year Established:
2012
Total Annual:
500,000,000-800,000,000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Company Overview : The company has an indoor warehouse of 5000 square meters and an open warehouse of 4000 square meters, which can fully meet the temporary turnover and phased storage of customers' steel pipe reservation. The subordinate processing plant has 6 sets of medium frequency h... Company Overview : The company has an indoor warehouse of 5000 square meters and an open warehouse of 4000 square meters, which can fully meet the temporary turnover and phased storage of customers' steel pipe reservation. The subordinate processing plant has 6 sets of medium frequency h...
Get in touch with us
Leave a Message, we will call you back quickly!