| Item | Sanicro 28 Stainless Steel Tube |
| Payment Term | 30%TT+70%TT / LC |
| Applications | Construction,Industry,boiler,Chemical |
| Condition | Soft / Hard |
| Appllication | heat exchanger/ chemical |
| Company Type | factory and trading |
| Ends | Plain End, Beveled End, Threaded End |
| Test | 100% NDT |
| Packing | Standard Sea-worthy Packing |
| Products | stainless steel pipe |
| Application | Industrial, Automotive, Construction |
| Secondary Or Not | Non-secondary |
| Color | natural color |
| Brand Name | TSING SHAN |
| Model Number | Sanicro 28 |
| Certification | ISO SGS MTC |
| Place of Origin | China |
View Detail Information
Explore similar products
ASTM A312 TP316L Stainless Steel Seamless Pipe 1.4404 Hollow Bar OD 90 ID 60 MM
Hollow Bar Seamless Sus316L OD45x28ID L3000 Mm ASTM A276 TP316L Stainless Steel
ASTM A790 S32750 2507 DIN1.4410 Super Duplex Steel Seamless Pipe 89*6*6000mm
Super Duplex 2507 Pipe And ASTM A790 S32750 Seamless Stainless Steel Pipe For
Product Specification
| Payment Terms | L/C, T/T | Supply Ability | 50000KGS |
| Delivery Time | 7 Days | Packaging Details | Export Packing |
| Package | Wooden Box, Steel Pallet, etc. | Third Party Inspection | BV,SGS,ASP |
| Item | Sanicro 28 Stainless Steel Tube | Payment Term | 30%TT+70%TT / LC |
| Applications | Construction,Industry,boiler,Chemical | Condition | Soft / Hard |
| Appllication | heat exchanger/ chemical | Company Type | factory and trading |
| Ends | Plain End, Beveled End, Threaded End | Test | 100% NDT |
| Packing | Standard Sea-worthy Packing | Products | stainless steel pipe |
| Application | Industrial, Automotive, Construction | Secondary Or Not | Non-secondary |
| Color | natural color | Brand Name | TSING SHAN |
| Model Number | Sanicro 28 | Certification | ISO SGS MTC |
| Place of Origin | China | ||
| High Light | ASTM B709 Nickel Alloy Tube ,Alloy 28 Nickel Alloy Tube ,Heat Exchanger Superalloy Tube | ||
Alloy 28 (UNS N08028, W. Nr. 1.4563, Sanicro 28) is a nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localise attack such as pitting and crevice corrosion. The alloy is especially resistant to sulphuric and phosphoric acid. Used for chemical processing, pollution control equipment, oil and gas well piping, nuclear fuel reprocessing, acid production and pickling equipment.
▪ Chemical and petrochemical processing industry
▪ Downhole service in deep sour gas wells.
Incoloy 28 Chemical Composition
| Element | Content (%) |
| Iron, Fe | 29-40.4 |
| Nickel, Ni | 30-34 |
| Chromium, Cr | 26-28 |
| Molybdenum, Mo | 3-4 |
| Manganese, Mn | ≤2.5 |
| Others | Remainder |
| Properties | Metric | Imperial |
| Tensile strength(annealed) | 500 MPa | 72.5 ksi |
| Yield strength(annealed) | 214 MPa | 31 ksi |
| Elongation at Break(Cold worked) | 15% | 50% |
| Modulus of Elasticity | 200 GPa | 29000 ksi |
| Hardness, Rockwell B | 80-90 | 80-90 |
| Hardness, Rockwell C | 33 | 33 |
| Incoloy 28 available sizes and specifications | |
| Grade | Incoloy 28 |
| Nickel plate | Thickness: 0.3mm - 150.0mm Width: 1000mm - 3000mm |
| Nickel strip/ nickel foil | Thickness: 0.02mm - 16.0mm Width: 5mm - 3000mm |
| Nickel coil | Thickness: 0.3mm - 16.0mm Width: 1000mm - 3000mm |
| Nickel pipe | Outside diameter: 6mm - 1219mm Thickness: 0.5mm - 100mm |
| Nickel Capillary Pipe | Outside diameter: 0.5mm - 6.0mm Thickness: 0.05mm - 2.0mm |
| Nickel bar | Diameter: Ф4mm - Ф600mm |
| Nickel wire rod | Diameter:Ф0.01mm - Ф6mm |
![]()
![]()
![]()
![]()
Q1: Do you accept the trial order ?
A1: Yes,if we have the exactly size in stock.we can delivery even 1 piece/meter .
Q2: Can I have free sample before making orders?
Company Details
Business Type:
Manufacturer
Year Established:
2012
Total Annual:
500,000,000-800,000,000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Company Overview : The company has an indoor warehouse of 5000 square meters and an open warehouse of 4000 square meters, which can fully meet the temporary turnover and phased storage of customers' steel pipe reservation. The subordinate processing plant has 6 sets of medium frequency h... Company Overview : The company has an indoor warehouse of 5000 square meters and an open warehouse of 4000 square meters, which can fully meet the temporary turnover and phased storage of customers' steel pipe reservation. The subordinate processing plant has 6 sets of medium frequency h...
Get in touch with us
Leave a Message, we will call you back quickly!