| Payment Terms | L/C,D/A,D/P,T/T,, |
| Supply Ability | 2,000 pcs/month |
| Packaging Details | Strong wooden box for Global shipping |
| Material | Silicon Nitride |
| Composition:SiC | >85% |
| Color | Black |
| Density | 3.20-3.26g/cm3 |
| Max. Service Temp | 1450℃ |
| Flexural Strength | 250MPa |
| Sample | Customizable |
| Chemical Stability | High |
| Apparent Porosity | 0-0.1% |
| Elastic Modulus | 300-320GPa |
| Compression Strength | >1500MPa |
| Vickers Hardness(HV0.5) | 15-16GPa |
| Thermal Conductivity | 20-25W/(m.k) |
| Specific Resistivity | 10^14Ω·cm |
| Brand Name | KEGU |
| Model Number | Customizable |
| Place of Origin | China |
View Detail Information
Explore similar products
Silicon Nitride Riser Tube with Extended Service Life, High-Temperature
High Thermal Shock Resistance Silicon Nitride Sealing Pipe and Si3N4 Sealing
Silicon Nitride Pouring Spoon and Crucible with Ultimate Thermal Shock
Black High Thermal Shock Resistance Customizable Silicon Nitride Ceramic for Non
Product Specification
| Payment Terms | L/C,D/A,D/P,T/T,, | Supply Ability | 2,000 pcs/month |
| Packaging Details | Strong wooden box for Global shipping | Material | Silicon Nitride |
| Composition:SiC | >85% | Color | Black |
| Density | 3.20-3.26g/cm3 | Max. Service Temp | 1450℃ |
| Flexural Strength | 250MPa | Sample | Customizable |
| Chemical Stability | High | Apparent Porosity | 0-0.1% |
| Elastic Modulus | 300-320GPa | Compression Strength | >1500MPa |
| Vickers Hardness(HV0.5) | 15-16GPa | Thermal Conductivity | 20-25W/(m.k) |
| Specific Resistivity | 10^14Ω·cm | Brand Name | KEGU |
| Model Number | Customizable | Place of Origin | China |
| High Light | High Thermal Conductivity Silicon Nitride Ceramic ,High Temperature Resistance Si3N4 Ceramic ,Customizable Ceramic Structural Part | ||
| Main component | 99%Al2O3 | S-SiC | ZrO2 | Si3N4 |
|---|---|---|---|---|
| Density (g/cm³) | 3.9 | 3.1 | 6 | 3.2 |
| Water Absorption (%) | 0 | 0.1 | 0 | 0.1 |
| Sinter Temperature (°C) | 1700 | 2200 | 1500 | 1800 |
| Property | 99%Al2O3 | S-SiC | ZrO2 | Si3N4 |
|---|---|---|---|---|
| Rockwell Hardness (HV) | 1700 | 2200 | 1300 | 1400 |
| Bend Strength (kgf/mm²) | 3500 | 4000 | 9000 | 7000 |
| Compression Intensity (Kgf/mm²) | 30000 | 20000 | 20000 | 23000 |
| Property | 99%Al2O3 | S-SiC | ZrO2 | Si3N4 |
|---|---|---|---|---|
| Maximum working temperature (°C) | 1500 | 1600 | 1300 | 1400 |
| Thermal expansion coefficient (0-1000°C) (/°C) | 8.0×10⁻⁶ | 4.1×10⁻⁶(0-500°C) 5.2×10⁻⁶(500-1000°C) |
9.5×10⁻⁶ | 2.0×10⁻⁶(0-500°C) 4.0×10⁻⁶(500-1000°C) |
| Thermal Shock resistance T(°C) | 200 | 250 | 300 | 400-500 |
| Thermal Conductivity W/m·k | 31 (25°C) 16 (300°C) |
100 | 3 | 25 |
| Property | 99%Al2O3 | S-SiC | ZrO2 | Si3N4 |
|---|---|---|---|---|
| Resisting rate of Volume (Ω·cm) | >10¹² (20°C) 10¹²-10¹³ (100°C) >10¹² (300°C) |
10⁶-10⁸ (20°C) | >10¹⁰ (20°C) | >10¹¹ (20°C, 100°C, 300°C) |
| Insulation Breakdown Intensity (KV/mm) | 18 | semiconductor | 9 | 17.7 |
| Dielectric Constant (1 MHz) (E) | 10 | - | 29 | 7 |
| Dielectric Dissipation (tg δ) | 0.4×10⁻³ | - | - | - |
Company Details
Business Type:
Manufacturer,Trading Company
Year Established:
2017
Ecer Certification:
Verified Supplier
.gtr-container-k7p9x2 { font-family: Verdana, Helvetica, "Times New Roman", Arial, sans-serif; color: #333; max-width: 100%; padding: 15px; margin: 0 auto; box-sizing: border-box; } @media (min-width: 768px) { .gtr-container-k7p9x... .gtr-container-k7p9x2 { font-family: Verdana, Helvetica, "Times New Roman", Arial, sans-serif; color: #333; max-width: 100%; padding: 15px; margin: 0 auto; box-sizing: border-box; } @media (min-width: 768px) { .gtr-container-k7p9x...
Get in touch with us
Leave a Message, we will call you back quickly!