China Nitronic 90 Cobalt Ni Based Superalloys ASTM A240 with high tensile strength
China Nitronic 90 Cobalt Ni Based Superalloys ASTM A240 with high tensile strength

  1. China Nitronic 90 Cobalt Ni Based Superalloys ASTM A240 with high tensile strength
  2. China Nitronic 90 Cobalt Ni Based Superalloys ASTM A240 with high tensile strength

Nitronic 90 Cobalt Ni Based Superalloys ASTM A240 with high tensile strength

  1. MOQ: 1000KGS
  2. Price: USD Negotiable
  3. Get Latest Price
Payment Terms T/T
Supply Ability 200 TONS per month
Delivery Time 7-15 days
Packaging Details Standard export packaging
TYPE OF MATERIAL cobalt-nickel base alloy
PRODUCT Nitronic90 cobalt-nickel base alloy steel plate
STANDARD ASTM A240, A182 or as appropriate
GRADE Nimonic90 / UNS N07090
Manufacturing process The steel melt shall be refined with AOD or equivalent.
Heat Treatment shall be supplied in the solution annealed/water quenched condition.
Surface Finish Descaled, White Pickled, and Passivated Condition.
Application areas Used in turbine engine blades, high temperature fasteners, clamps, seals and elastic components.
Brand Name ABOOM
Model Number Nitronic90
Certification EN 10204 Type 3.1
Place of Origin CHINA

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 200 TONS per month
Delivery Time 7-15 days Packaging Details Standard export packaging
TYPE OF MATERIAL cobalt-nickel base alloy PRODUCT Nitronic90 cobalt-nickel base alloy steel plate
STANDARD ASTM A240, A182 or as appropriate GRADE Nimonic90 / UNS N07090
Manufacturing process The steel melt shall be refined with AOD or equivalent. Heat Treatment shall be supplied in the solution annealed/water quenched condition.
Surface Finish Descaled, White Pickled, and Passivated Condition. Application areas Used in turbine engine blades, high temperature fasteners, clamps, seals and elastic components.
Brand Name ABOOM Model Number Nitronic90
Certification EN 10204 Type 3.1 Place of Origin CHINA
High Light Cobalt ni based superalloys ,Nitronic 90 ni based superalloys ,Nitronic 90 ASTM A240

Nitronic90 Cobalt Superalloys Steel Plate Custom N07090 ASTM A240 A182

 

Nitronic90 cobalt-nickel base alloy steel plate custom N07090

 

United States: UNS N07090
United Kingdom: Nitronic90

 

This alloy is an age-strengthened cobalt-nickel-based deformed high-temperature alloy, which contains a higher amount of cobalt and various strengthening elements. The alloy has a high tensile strength and creep resistance, good performance and corrosion resistance at 815-870 ° C 3. High fatigue strength and good formability and weldability under repeated action of cold and heat. Used in turbine engine blades, high temperature fasteners, clamps, seals and elastic components.

 

Nitronic90

CHEMICAL ANALYSIS
C Carbon 0.20 max
Mn Manganese 1.00 max
Si Silicon 1.00 max
Fe Iron 1.50 max
Cr Chromium 18.00 – 21.00
Co Cobalt 15.0 – 21.0
Al Aluminum 1.0 – 2.0
Ti Titanium 2.0 – 3.0
S Sulfur 0.015 max
Ni Nickel Balance

GENERAL CHARACTERISTICS OF NIMONIC ALLOY 90

This is a precipitation-hardenable nickel-chromium-cobalt alloy with strengthening additions of titanium and aluminum. The alloy has high stress-rupture strength and is creep resistant to 1690ºF(920ºC.)

APPLICATIONS

Nitronic90 alloy is used in extreme stress applications such as turbine blades, hot working tools, exhaust reheaters and high-temperature springs.

FORGING

The alloy should be forged between 2100 and 1850ºF (1150 and 1010ºC) after which process it may be air cooled or water quenched, depending upon the size and intricacy of the forged part.

HEAT TREATMENT

For bar material the following heat treatment is recommended :

Solution treat at 1975ºF (1080ºC) for 8 hours and air cool or oil/water quench.

Precipitation treat at 1290ºF (700ºC) for 16hours and air cool.

MACHINABILITY

The alloy should be in the fully heat-treated condition prior to machining operations. Machining should be carried out under strict conditions as specified by Special Metals Corporation, who should be consulted regarding detailed procedures.

WELDABILITY

Nitronic90 alloy sheet may be welded by any resistance process. For material up to 5mm (0.2in.) thick, TIG or MIG processes are satisfactory. Above this thickness micro-cracking may occur in the weld and the heat-affected zone. Electron beam, friction, inertia and flash-butt welding are all satisfactory for material over 5 mm thick.

Welding should be done on solution-treated material and post-weld heat treatment is necessary to achieve optimum properties.

 

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Employee Number:

    >100

  • Ecer Certification:

    Active Member

                      Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...                       Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...

+ Read More

Get in touch with us

  • Reach Us
  • Shanghai Aboom Metal prodcut co.,ltd
  • NO.161 XingFei Road ,Songjiang Disrict,Shanghai 201601, P.R.CHINA
  • http://www.superduplexss.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement