China UNS N07090 Nimonic 90 Cobalt Based Superalloys For Turbine Blades
China UNS N07090 Nimonic 90 Cobalt Based Superalloys For Turbine Blades

  1. China UNS N07090 Nimonic 90 Cobalt Based Superalloys For Turbine Blades
  2. China UNS N07090 Nimonic 90 Cobalt Based Superalloys For Turbine Blades

UNS N07090 Nimonic 90 Cobalt Based Superalloys For Turbine Blades

  1. MOQ: 1000kgs
  2. Price: USD Negotiable
  3. Get Latest Price
Payment Terms T/T
Supply Ability 200 TONS PER MONTH
Delivery Time 7-15dyas
Packaging Details Bare packing/bundle packing with woven bag/wooden or steel frame crate packing/plastic cap protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.
TYPE OF MATERIAL nickel-chromium-cobalt base alloy
PRODUCT Nimonic90 / UNS N07090 / W. Nr.2.4632 alloy seamless pipe
STANDARD ASME SB 167
GRADE Nimonic90 / UNS N07090 / W. Nr.2.4632
Manufacturing process The steel melt shall be refined with AOD or equivalent.
Type Of Tube Straight Pipe, U Bend Pipe , Coil Pipe
Surface Finish Pickled And Annealed, Bright Annealed, Polished
Brand Name ABOOM
Model Number Nimonic90
Certification EN 10204 Type 3.1
Place of Origin CHINA

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 200 TONS PER MONTH
Delivery Time 7-15dyas Packaging Details Bare packing/bundle packing with woven bag/wooden or steel frame crate packing/plastic cap protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.
TYPE OF MATERIAL nickel-chromium-cobalt base alloy PRODUCT Nimonic90 / UNS N07090 / W. Nr.2.4632 alloy seamless pipe
STANDARD ASME SB 167 GRADE Nimonic90 / UNS N07090 / W. Nr.2.4632
Manufacturing process The steel melt shall be refined with AOD or equivalent. Type Of Tube Straight Pipe, U Bend Pipe , Coil Pipe
Surface Finish Pickled And Annealed, Bright Annealed, Polished Brand Name ABOOM
Model Number Nimonic90 Certification EN 10204 Type 3.1
Place of Origin CHINA
High Light Nimonic 90 cobalt superalloys ,UNS N07090 cobalt superalloys ,UNS N07090 co based superalloys

ASME SB 167 Nickel Chromium Cobalt Alloy UNS N07090 Nimonic90 / W. Nr.2.4632

 

Nimonic90 / UNS N07090 / W. Nr.2.4632 alloy seamless pipe customization

 

Nimonic 90*(UNS N07090/W. Nr.2.4632)

Introduction

NIMONIC 90 (UNS N07090/W. Nr. 2.4632) is a wrought nickel-chromium-cobalt base alloy strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 920°C

 

Application

The alloy is used for turbine blades, discs, forgings, ring sections and hot-working tools. Also used to make Aerospace fasteners.

Equal grades

GH4090
Nickel Alloy 90
UNS N07090
Werkstoff Nr. 2.4632
Werkstoff Br. 2.4969
NiCr20Co18Ti

 

Chemical composition

C≤0.13 Cr=18.00~21.00 Co=15.00~21.00 Al=1.00~2.00
Ti=2.00~3.00 Fe≤1.50 Zr≤0.0150 B≤0.020
Si≤0.80 Mn≤0.40 Si≤0.015 P≤0.020
Cu≤0.200 Ni=Remainder    

 

Standard

AMS 5829

Forms of product available

Plate, sheet, strip, bar, wire, rod, pipe, tube, forging.

Delivery

Available on request


Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Employee Number:

    >100

  • Ecer Certification:

    Active Member

                      Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...                       Shanghai Aboom Metal prodcut co.,ltd mainly produces and sells super duplex stainless steel, special super austenitic stainless steel and high temperature alloys, nickel-based alloys, corrosion-resistant alloys, precisio...

+ Read More

Get in touch with us

  • Reach Us
  • Shanghai Aboom Metal prodcut co.,ltd
  • NO.161 XingFei Road ,Songjiang Disrict,Shanghai 201601, P.R.CHINA
  • http://www.superduplexss.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement