China factories

Chat Now Send Email
China factory - Beijing Tonghe Testing Machine Co., ltd

Beijing Tonghe Testing Machine Co., ltd

  • China,Beijing ,Beijing
  • Verified Supplier
  1. Home
  2. Products
  3. About Us
  4. Contact Us

Leave a Message

we will call you back quickly!

Submit Requirement
China Industrial Differential Scanning Calorimeter Featuring Widescreen Touch
China Industrial Differential Scanning Calorimeter Featuring Widescreen Touch

  1. China Industrial Differential Scanning Calorimeter Featuring Widescreen Touch
  2. China Industrial Differential Scanning Calorimeter Featuring Widescreen Touch

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch

  1. MOQ: 1 set
  2. Price:
  3. Get Latest Price
Temperature control mode Heating, cooling, constant temperature
Payment Terms L/C,D/A,D/P,T/T,Western Union
Supply Ability 20 sets per month
Delivery Time 10~15 work days
Packaging Details Standard export wooden box
Temperature resolution 0.01 ℃
DSC range 0 ~ + 500 mw
DSC sensitivity 0.01 mW
DSC resolution 0.01 mW
Heating rate 0.1~40℃/min
Product name Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement
Cooling rate 0.1~20℃/min
Brand Name TH
Model Number DSC-ZS5
Certification ISO9001 CE
Place of Origin BEIJING, CHINA

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Temperature control mode Heating, cooling, constant temperature Payment Terms L/C,D/A,D/P,T/T,Western Union
Supply Ability 20 sets per month Delivery Time 10~15 work days
Packaging Details Standard export wooden box Temperature resolution 0.01 ℃
DSC range 0 ~ + 500 mw DSC sensitivity 0.01 mW
DSC resolution 0.01 mW Heating rate 0.1~40℃/min
Product name Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement Cooling rate 0.1~20℃/min
Brand Name TH Model Number DSC-ZS5
Certification ISO9001 CE Place of Origin BEIJING, CHINA
High Light Industrial differential scanning calorimeter with touch interface ,Polymer oxidation induction period calorimeter ,Widescreen DSC for accurate measurements
Industrial Differential Scanning Calorimeter with Widescreen Touch Interface
This Differential Scanning Calorimeter (DSC) features a touchscreen interface specifically engineered for oxidation induction period (OIT) testing of polymeric materials. It supports one-key operation and full software automation, streamlining testing workflows and ensuring consistent, error-free operation.
Standards Compliance
This instrument fully complies with the following international and national standards:
  • GB/T 19466.2-2009 / ISO 11357-2:1999
  • GB/T 19466.3-2009 / ISO 11357-3:1999
  • GB/T 19466.6-2009 / ISO 11357-6:1999
Key Features
  • Industrial-Grade Widescreen Touch Interface: Information-rich display showing comprehensive real-time data including set temperature, sample temperature, gas flow rates, differential thermal signal, and switch statuses
  • Universal USB Communication Interface: High universality with reliable data transmission and built-in self-recovering connection functionality
  • Compact Furnace with Adjustable Thermal Rates: Supports stepless adjustment of heating and cooling rates for various polymeric material OIT tests
  • Optimized Installation & Anti-Contamination Design: Mechanical fastening method eliminates contamination of differential thermal signal
  • Efficient Heating & Cooling System: Electric heating with circulating cooling water, compact structure with small footprint
  • High-Precision Temperature Control: Dual temperature probes and specialized control technology for excellent repeatability
  • Automatic Gas Channel Switching: Fast switching between two gas channels with short stabilization time
  • Standard Reference Samples: Includes calibration materials for temperature and enthalpy coefficients
  • Versatile Software Compatibility: Supports all screen resolutions and multiple Windows operating systems
  • Customizable Automated Operation: Supports user-edited device operation modes with dozens of configurable instructions
  • Fully Enclosed Protective Structure: Prevents foreign object entry, avoids furnace contamination, and reduces maintenance
Technical Specifications
Temperature Range 0℃ ~ 500℃
Temperature Resolution 0.01℃
Heating Rate 0.1 ~ 40℃/min
Cooling Rate 0.1 ~ 20℃/min
Calorimetric Resolution 100%
Constant Temperature Range 5℃ ~ 500℃
Temperature Control Modes Heating, cooling, constant temperature
DSC Range 0 ~ ±500mW
DSC Resolution 0.01mW
DSC Sensitivity 0.01mW
Working Power AC 220V 50Hz 300W or other
Atmosphere Control Two-channel automatic control (nitrogen and oxygen)
Gas Flow Range 0-200mL/min
Gas Pressure 0.2MPa
Gas Flow Accuracy 0.2mL/min
Crucible Type Aluminium crucible Φ6.6*3mm (Diameter * Height)
Calibration Standard Includes standard materials (indium, tin, zinc)
Data Interface Standard USB interface
Display Mode 7-inch touch screen
Output Mode Computer and printer
Standard Configuration
DSC Machine 1 set
Aluminium Crucibles 300 pieces
Power Cords and USB Cable Each one
CD (Software & Operations Video) One
Soft-key One
Oxygen and Nitrogen Airways Each 5m
Operation Manual One
Standard Samples (Indium, Tin, Zinc) Each one
Tweezer and Medicine Spoon Each one
Custom Pressure Reducing Valve Joint and Quick Joint Two
Fused Glass Fuses Four
External Circulation Thermostat Sink One
Water Pipe One
Furnace Bracket
Industrial DSC furnace bracket and structural components
Software Interface
DSC software interface showing temperature control and data analysis DSC software data visualization and measurement parameters DSC software thermal analysis curves and results display DSC software automated testing configuration interface

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Exporter

  • Employee Number:

    50~60

  • Ecer Certification:

    Verified Supplier

 Beijing Tonghe Testing Instruments Co., Ltd. Profile 1. Company Foundation and Positioning: Beijing Tonghe Testing Instrument Co., Ltd. was founded by a core team with over 20 years of experience in material testing and testing machine R&D. With mature technical solutions and a global...  Beijing Tonghe Testing Instruments Co., Ltd. Profile 1. Company Foundation and Positioning: Beijing Tonghe Testing Instrument Co., Ltd. was founded by a core team with over 20 years of experience in material testing and testing machine R&D. With mature technical solutions and a global...

+ Read More

Get in touch with us

  • Reach Us
  • Beijing Tonghe Testing Machine Co., ltd
  • No. 1, Fengguan Road, Fengtai District, Beijing
  • https://www.utm-machine.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement